[1]赵新伟,王高峰,杨锋平,等.管道环焊缝修复用高强度B型套筒及应用关键技术[J].油气储运,2022,41(10):1141-1149.[doi:10.6047/j.issn.1000-8241.2022.10.003]
 ZHAO Xinwei,WANG Gaofeng,YANG Fengping,et al.High-strength type-B sleeve for pipeline girth weld repair and its key application technology[J].Oil & Gas Storage and Transportation,2022,41(10):1141-1149.[doi:10.6047/j.issn.1000-8241.2022.10.003]
点击复制

管道环焊缝修复用高强度B型套筒及应用关键技术

参考文献/References:

[1] 王海涛,李仕力,陈杉,罗艳龙,张雪涛,周少坤.高钢级天然气管道环焊缝断裂问题探讨[J].石油管材与仪器,2020,6(2):49-52. WANG H T, LI S L, CHEN S, LUO Y L, ZHANG X T, ZHOU S K. Fracture of gas pipeline girth welds with high grade steel[J].Petroleum Tubular Goods & Instruments, 2020, 6(2): 49-52.
[2] 李亮,黄磊,许彦,丰振军,聂向晖,刘迎来.某X70钢级输气管道环焊缝裂纹产生原因分析[J].热加工工艺,2022,51(7):143-147. LI L, HUANG L, XU Y, FENG Z J, NIE X H, LIU Y L. Analysis on causes of cracks in girth weld of a X70 steel gas transmission pipeline[J]. Hot Working Technology, 2022, 51(7):143-147.
[3] 余东亮,杨川,吴东容,王爱玲,黄辉,贾彬,等. X80管道环焊缝缺陷钢质环氧套筒补强试验[J].油气储运,2021,40(9):997-1007. YU D L, YANG C, WU D R, WANG A L, HUANG H, JIA B, et al. Reinforcement test of epoxy-filled steel sleeves for girth weld defects of X80 pipelines[J]. Oil & Gas Storage and Transportation, 2021, 40(9): 997-1007.
[4] 杨锋平,许彦,曹国飞,吴明畅. X80管线钢环焊缝力学性能及缺陷成因分析[J].压力容器,2020,37(1):68-73. YANG F P, XU Y, CAO G F, WU M C. Analysis of key mechanical properties and defect causes of X80 girth weld[J]. Pressure Vessel Technology, 2020, 37(1): 68-73.
[5] 江金旭,张宏,顾磊,张东,吴锴,刘啸奔.高钢级管道环焊缝表观断裂韧性影响因素数值模拟[J].油气储运,2022,41(3):281-287. JIANG J X, ZHANG H, GU L, ZHANG D, WU K, LIU X B. Numerical simulation on influencing factors of apparent fracture toughness of girth welds on high-grade steel pipelines[J]. Oil &Gas Storage and Transportation, 2022, 41(3): 281-287.
[6] 帅健,王旭,张银辉,武旭.高钢级管道环焊缝主要特征及安全性评价[J].油气储运,2020,39(6):623-631. SHUAI J, WANG X, ZHANG Y H, WU X. Main characteristics and safety assessment of girth welds in high grade steel pipelines[J]. Oil & Gas Storage and Transportation, 2020, 39(6):623-631.
[7] 杨悦,张宏,刘啸奔,吴锴,隋永莉,杨叠.焊接材料强度对高钢级管道环焊缝应变能力的影响[J].油气储运,2022,41(1):48-54. YANG Y, ZHANG H, LIU X B, WU K, SUI Y L, YANG D. Influence of welding material strength on strain capacity of girth welds in high-grade steel pipelines[J]. Oil & Gas Storage and Transportation, 2022, 41(1): 48-54.
[8] 任俊杰,马卫锋,惠文颖,罗金恒,王珂,马秋荣,等.高钢级管道环焊缝断裂行为研究现状及探讨[J].石油工程建设,2019, 45(1):1-5. REN J J, MA W F, HUI W Y, LUO J H, WANG K, MA Q R, et al. Research status and prospect on fracture behaviour of butt girth welds in high grade steel pipelines[J]. Petroleum Engineering Construction, 2019, 45(1): 1-5.
[9] 李荣光,张巍,赵振,于憬,汤斌,孙旭,等.高钢级管道环焊缝缺陷修复技术探讨[J].油气储运,2020,39(3):307-312,360. LI R G, ZHANG W, ZHAO Z, YU J, TANG B, SUN X, et al. Discussion on repair technology of girth weld defects of high-grade steel pipelines[J]. Oil & Gas Storage and Transportation, 2020, 39(3): 307-312, 360.
[10] 李荣光,冯庆善,王学力,刘悦,王春明,陈哲,等. B型全封闭钢质套筒修复技术改进[J].油气储运,2010,29(10):755-758. LI R G, FENG Q S, WANG X L, LIU Y, WANG C M, CHEN Z, et al. Improvement on remediation technology for type B full-encirclement steel sleeves[J]. Oil & Gas Storage and Transportation, 2010, 29(10): 755-758.
[11] GUEST S, DYCK J, EGBEWANDE A, MACKENZIE R, SADOWSKI M. Design of in-service repair welding procedures for operating pipelines: critical assessment of variables affecting restraint level and heat-affected zone microstructures of vintage pipelines[C]. Calgary: 2016 11th International Pipeline Conference, 2016: V003T05A041.
[12] ALIAN A R, SHAZLY M, MEGAHED M M. 3D finite element modeling of in-service sleeve repair welding of gas pipelines[J]. International Journal of Pressure Vessels and Piping, 2016, 146: 216-229.
[13] TRONSKAR J P, T?RNQVIST R, GUAN O H, BRUCE W A. “Live” repair of gas pipeline with deep girth weld crack[C]. Boston: ASME 2015 Pressure Vessels and Piping Conference, 2015: V06BT06A044.
[14] WANG Y, WANG L J, DI X J, SHI Y T, BAO X W, GAO X M. Simulation and analysis of temperature field for in-service multi-pass welding of a sleeve fillet weld[J]. Computational Materials Science, 2013, 68: 198-205.
[15] 李琴,唐崇尧,常维纯,郭旭,李德杰,徐兆东.焊接顺序对X80钢管道B型套筒熔化极活性气体保护电弧焊接残余应力的影响[J].机械工程材料,2022,46(3):83-88,94.
LI Q, TANG C Y, CHANG W C, GUO X, LI D J, XU Z D.Effect of metal active gas arc welding sequence on welding residual stress of X80 steel pipe B-type sleeve[J]. Materials for Mechanical Engineering, 2022, 46(3): 83-88, 94.
[16] CRAPPS J M, YUE X, BERLIN R A, SUAREZ H A, PRIBYTKOV P A, VYVIAL B A, et al. Strain-based pipeline repair via type B sleeve[C]. San Francisco: The 27th International Ocean and Polar Engineering Conference, 2017:ISOPE-I-17-693.
[17] 胥聪敏,罗立辉,周会萍,裴廷刚,李丽锋,罗金恒. B型套筒焊接对X80管线钢性能的影响[J].材料保护,2019,52(6):149-156. XU C M, LUO L H, ZHOU H P, PEI T G, LI L F, LUO J H. Influence of B-type sleeve welding on the performance of X80 pipeline steel[J]. Materials Protection, 2019, 52(6): 149-156.
[18] 成志强,胡聪,段金伟,吕志伟,杨涛. B型套筒角焊缝力学性能模拟实验[J].西南石油大学学报(自然科学版),2021,43(6):111-118. CHENG Z Q, HU C, DUAN J W, LYU Z W, YANG T. Simulation test of mechanical properties of B-type sleeve fillet weld[J]. Journal of Southwest Petroleum University (Science &Technology Edition), 2021, 43(6): 111-118.
[19] 吕晓春,秦建,杜兵,徐良,王琪昭.回火焊道焊接技术的研究进展[J].焊接,2014(7):16-21,73. LYU X C, QIN J, DU B, XU L, WANG Q Z. Research progress of temper bead welding technology[J]. Welding & Joining, 2014(7): 16-21, 73.
[20] ALORAIER A S, JOSHI S, ASADI M, ALENA R G, GOLDAK J A. Microstructural and hardness modeling: effect of multiple bead deposition in temper bead welding technique[J]. International Journal of Energy & Technology, 2010, 2(16): 1-11.

相似文献/References:

[1]隋永莉,吴宏.我国长输油气管道自动焊技术应用现状及展望[J].油气储运,2014,33(9):913.[doi:10.6047/j.issn.1000-8241.2014.09.001]
 SUI Yongli,WU Hong.Current and future applications of automatic welding technology for long-distance oil/gas pipeline in China[J].Oil & Gas Storage and Transportation,2014,33(10):913.[doi:10.6047/j.issn.1000-8241.2014.09.001]
[2]王婷,杨辉,冯庆善,等.油气管道环焊缝缺陷内检测技术现状与展望[J].油气储运,2015,34(7):694.[doi:10.6047/j.issn.1000-8241.2015.07.003]
 WANG Ting,YANG Hui,FENG Qingshan,et al.Current status and prospect of inline inspection technologies for defects in girth weld of oil and gas pipeline[J].Oil & Gas Storage and Transportation,2015,34(10):694.[doi:10.6047/j.issn.1000-8241.2015.07.003]
[3]周亚薇 张振永.中俄东线天然气管道环焊缝断裂韧性设计[J].油气储运,2018,37(预出版):1.
 ZHOU Yawei,ZHANG Zhenyong.The design for the fracture toughness of girth weld in Russia-China Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2018,37(10):1.
[4]张振永 张文伟 周亚薇 薄国公.中俄东线OD 1 422 mm 埋地管道的断裂控制设计[J].油气储运,2017,36(预出版):1.
 ZHANG Zhenyong,ZHANG Wenwei,ZHOU Yawei,et al.The fracture control design of the OD 1 422 mm buried pipeline in China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(10):1.
[5]张振永,张文伟,周亚薇,等.中俄东线OD 1 422 mm 埋地管道的断裂控制设计[J].油气储运,2017,36(9):1059.[doi:10.6047/j.issn.1000-8241.2017.09.013]
 ZHANG Zhenyong,ZHANG Wenwei,ZHOU Yawei,et al.The fracture control design of the OD 1 422 mm buried pipeline in China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(10):1059.[doi:10.6047/j.issn.1000-8241.2017.09.013]
[6]帅健,孔令圳.高钢级管道环焊缝应变能力评价[J].油气储运,2017,36(12):1368.[doi:10.6047/j.issn.1000-8241.2017.12.004]
 SHUAI Jian,KONG Lingzhen.Evaluation on strain capacity of girth welds in high-grade pipelines[J].Oil & Gas Storage and Transportation,2017,36(10):1368.[doi:10.6047/j.issn.1000-8241.2017.12.004]
[7]周亚薇,张振永.中俄东线天然气管道环焊缝断裂韧性设计[J].油气储运,2018,37(10):1174.[doi:10.6047/j.issn.1000-8241.2018.10.015]
 ZHOU Yawei,ZHANG Zhenyong.The design for the fracture toughness of girth weld in China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2018,37(10):1174.[doi:10.6047/j.issn.1000-8241.2018.10.015]
[8]吕新昱 高媛 刘全利 薛岩 李新文 肖健 刘宝强 李维.中俄东线天然气管道AUT检测技术质量控制及管理[J].油气储运,2020,39(中俄东线):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
 LYU Xinyu,GAO Yuan,LIU Quanli,et al.Quality control and management of AUT technology for China-Russia Eastern Gas Pipeline [J].Oil & Gas Storage and Transportation,2020,39(10):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
[9]张振永.高钢级大口径天然气管道环焊缝安全提升设计关键[J].油气储运,2020,39(中俄东线):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
 ZHANG Zhenyong.Key factors for safety improvement design of girth weld in high-gradelarge diameter natural gas pipelines[J].Oil & Gas Storage and Transportation,2020,39(10):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
[10]帅健 王旭 张银辉 武旭.高钢级管道环焊缝主要特征及安全性评价[J].油气储运,2020,39(06):623.[doi:10.6047/j.issn.1000-8241.2020.06.003]
 SHUAI Jian,WANG Xu,ZHANG Yinhui,et al.Main characteristics and safety assessment of girth welds in high grade steel pipelines[J].Oil & Gas Storage and Transportation,2020,39(10):623.[doi:10.6047/j.issn.1000-8241.2020.06.003]

备注/Memo

赵新伟,男,1969年生,教授级高工,2004年博士毕业于西安交通大学材料科学与工程专业,现主要从事油气输送管与管道完整性技术研究工作。地址:陕西省西安市雁塔区锦业二路89号, 710077。电话:13609265830。Email:zhaoxinwei001@cnpc.com.cn
基金项目:中国石油管道有限责任公司2019年科技计划项目“天然气管道环焊缝修复用B型套筒维抢修关键技术及换管焊接工艺优化研究”,2019E-23-0501。
(收稿日期:2022-06-21;修回日期:2022-08-12;编辑:张腾)

更新日期/Last Update: 2022-10-25