[1]江怡舟 田大庆 杨辉.基于无缝表征模型的点蚀管道剩余强度评估[J].油气储运,2020,39(09):997-1001.[doi:10.6047/j.issn.1000-8241.2020.09.005]
 JIANG Yizhou,TIAN Daqing,YANG Hui.Residual strength assessment of pipelines with pitting corrosion based on non-discrete characterization model[J].Oil & Gas Storage and Transportation,2020,39(09):997-1001.[doi:10.6047/j.issn.1000-8241.2020.09.005]
点击复制

基于无缝表征模型的点蚀管道剩余强度评估

参考文献/References:

[1] ABE H,MATSUO K,TAKAHASHI K. Estimation of remaining fatigue life for elbow pipe subjected to cyclic overload[C]. Toronto:ASME 2012 Pressure Vessels and Piping Conference,2012:45-50.
[2] HOANG V T,龙伟,刘华国,李金刚. 基于有限元的含均匀腐蚀 缺陷油气管道剩余强度[J]. 油气储运,2018,37(2):157-161. HOANG V T,LONG W,LIU H G,LI J G. Research on residual strength of metallic oil and gas pipelines with uniform corrosion defects based on finite element method[J]. Oil & Gas Storage and Transportation,2018,37(2):157-161.
[3] 江怡舟,HOANG V T,田大庆. 点蚀管道剩余强度评价的协同 评估综合影响因子[J]. 腐蚀与防护,2020,41(2):65-68. JIANG Y Z,HOANG V T,TIAN D Q. Synthetical impact factor for synergy assessing residual strength of pipelines with pitting corrosion[J]. Corrosion & Protection,2020,41(2): 65-68.
[4] 王猛,赵冬岩. 基于DNV-RP-F101 规范的腐蚀海底管道强度评 估研究[J]. 海洋工程装备与技术,2017,4(5):276-280. WANG M,ZHAO D Y. Strength assessment on corroded subsea pipeline based on the code of DNV-RP-F101[J]. Ocean Engineering Equipment and Technology,2017,4(5): 276-280.
[5] 王予东,肖志刚. 在役含缺陷油气管道的安全评价准则[J]. 油气 储运,2013,32(6):587-589. WANG Y D,XIAO Z G. Safety evaluation standards for inservice oil and gas pipelines with defects[J]. Oil & Gas Storage and Transportation,2013,32(6):587-589.
[6] 何东升,张鹏,张丽萍. API 579 与B31G 剩余强度评价的保守 性分析[J]. 油气储运,2008,27(1):36-40. HE D S,ZHANG P,ZHANG L P. Conservative analysis on the remaining strength assessment of corroded pipeline for ASME B31G and API 579[J]. Oil & Gas Storage and Transportation, 2008,27(1):36-40.
[7] 龙伟,宋恩奎,林思建. 基于缺陷失效仿真路径压力容器的安全 裕度与剩余寿命研究[J]. 四川大学学报(工程科学版),2012, 44(4):204-208. LONG W,SONG E K,LIN S J. Study on the residual life and the safety margin of pressure vessel based on the defect failure simulation path[J]. Journal of Sichuan University(Engineering Science Edition),2012,44(4):204-208.
[8] 龙伟,严佳兵,李炎炎,刘华国,黄吉民. 基于缺陷安全衰减路径 仿真的含埋藏裂纹压力容器剩余寿命研究[J]. 工程科学与技 术,2018,50(5):239-243. LONG W,YAN J B,LI Y Y,LIU H G,HUANG J M. Study on the residual life of pressure vessel with immerged cracks based on defect security attenuation path simulation[J]. Advanced Engineering Sciences,2018,50(5):239-243.
[9] 徐寅平,段庆全,张宏. 基于API 579 准则的含点腐蚀管道剩余 强度分析[J]. 腐蚀与防护,2016,37(9):748-752. XU Y P,DUAN Q Q,ZHANG H. Residual strength evaluation of pipeline with pitting corrosion based on API 579 criterion[J]. Corrosion & Protection,2016,37(9):748-752.
[10] 崔晔晖,曾祥国,李洋,盛鹰. 基于API 579 准则对弯管腐蚀数 值模拟的分析[J]. 包钢科技,2017,43(2):53-57. CUI Y H,ZENG X G,LI Y,SHENG Y. Numerical simulation analysis of elbow erosion based on API 579 criterion[J]. Science & Technology of Baotou Steel,2017,43(2):53-57.
[11] 吴晓宇,段庆全,周雪静,张宏. 基于API 579 的受附加载荷管 道局部腐蚀评价[J]. 石油工业技术监督,2015,31(7):42-47. WU X Y,DUAN Q Q,ZHOU X J,ZHANG H. Local corrosion assessment of the pipeline subjecting to additional loads based on API 579[J]. Technology Supervision in Petroleum Industry, 2015,31(7):42-47.
[12] 冯胜,曲伟首,王海锋,金磊,张传旭. 含腐蚀缺陷海底管道安 全评价方法比较[J]. 石油化工设备,2020,49(1):10-16. FENG S,QU W S,WANG H F,JIN L,ZHANG C X. Safety evaluation methods comparison of submarine pipelines with corrosion defects[J].Petro-Chemical Equipment,2020,49(1): 10-16.
[13] 张健,孙奇北,王文燕,杜明超,伊岩,张保存. 天然气管道 缺陷模型的建立及有限元分析[J]. 石油机械,2019,47(4): 129-134. ZHANG J,SUN Q B,WANG W Y,DU M C,YI Y,ZHANG B C. Modeling and finite element analysis of natural gas pipeline defect[J]. China Petroleum Machinery,2019,47(4):129-134.
[14] 韩烨,孙伟栋,席少龙,孙霄,阮伟东. 含腐蚀缺陷占压管道的 安全评估[J]. 油气储运,2019,38(2):137-144. HAN Y,SUN W D,XI S L,SUN X,RUAN W D. Safety assessment on buried pipeline subjected to ground load andcorrosion defect[J]. Oil & Gas Storage and Transportation, 2019,38(2):137-144.
[15] XU C,LONG W,TIAN D Q,LIN S J. The method of the residual life prediction of pressure vessel defect based on defect failure rate inflection point[J]. Applied Mechanics and Materials,2013,423/424/425/426:1905-1909.
[16] 宁朝阳,黎佳. 基于失效路径理论的压力容器裂纹缺陷安全评 定[J]. 化工机械,2015,42(3):311-313. NING Z Y,LI J. Safety assessment of pressure vessel cracks based on failure paths theory[J]. Chemical Engineering & Machinery,2015,42(3):311-313.
[17] 谢阳,龙伟,赵波,刘华国. 压力容器缺陷安全评定研究进展和 衰减路径速度积方法[J]. 机械,2019,46(11):8-15,28. XIE Y,LONG W,ZHAO B,LIU H G. Research advance on safety assessment of pressure vessel defects and the method based on the product of attenuation path and velocity[J]. Machinery, 2019,46(11):8-15,28.
[18] 徐磊,龙伟,林思建. 基于裂纹失效路径的压力容器剩余寿命 预测新方法[J]. 科学技术与工程,2016,16(28):190-194. XU L,LONG W,LIN S J. New method of residual life prediction for pressure vessel surface crack defects based on the crack failure path[J]. Science Technology and Engineering, 2016,16(28):190-194.
[19] 林思建,龙伟,田大庆,廖俊必. 含点蚀缺陷金属压力管道剩余 强度的无缝表征模型[J]. 四川大学学报(工程科学版),2013, 45(6):184-187. LIN S J,LONG W,TIAN D Q,LIAO J B. Non-discrete characterization model of residual strength of metal pressure pipeline with pitting corrosion[J]. Journal of Sichuan University (Engineering Science Edition),2013,45(6):184-187.
[20] LIN S J,LONG W,TIAN D Q,LIAO J B. A new fatigue damage accumulation model considering loading history and loading sequence based on damage equivalence[J]. International Journal of Damage Mechanics,2018,27(5):707-728.
[21] 甘芳吉,万正军,罗航,宋康,廖俊必. 基于场指纹法的金属 管道小腐蚀坑的监测方法[J]. 仪器仪表学报,2013,34(9): 2087-2094. GAN F J,WAN Z J,LUO H,SONG K,LIAO J B. Monitoring method for small corrosion pits of metal pipeline based on field signature method[J]. Chinese Journal of Scientific Instrument, 2013,34(9):2087-2094.
[22] 李金刚,林思建,龙伟,徐磊. 基于FSM 无损检测的金属管道 均匀腐蚀剩余寿命预测[J]. 表面技术,2016,45(3):7-11. LI J G,LIN S J,LONG W,XU L. Residue life prediction for metal pipe with uniform corrosion based on no damage detection using field signature method[J]. Surface Technology,2016,45(3): 7-11.
[23] 江怡舟,田大庆,周博. 基于无缝表征模型的油气输送管道安 全裕度与剩余寿命在线监测平台研制[J]. 机械,2019,46(5): 42-46,51. JIANG Y Z,TIAN D Q,ZHOU B. Development on residual life and safety margin online monitoring platform of oil and gas pipelines with pitting corrosion based on non-discrete characterization model[J]. Machinery,2019,46(5):42-46,51.

相似文献/References:

[1]黄春芳 陈燕 周芳 黄月 吴州阳 杨松 王自发. 石油天然气管道站内管道爆破吹扫[J].油气储运,2012,31(12):934.[doi:10.6047/j.issn.1000-8241.2012.06.016]
 Huang Chunfang,Chen Yan,Zhou Fang,et al. Bursting purge method in stations of oil and gas pipeline[J].Oil & Gas Storage and Transportation,2012,31(09):934.[doi:10.6047/j.issn.1000-8241.2012.06.016]
[2]戴联双,汤长江,冯治中,等.油气管道恐怖袭击风险评估方法与应用[J].油气储运,2011,30(05):337.[doi:10.6047/j.issn.1000-8241.2011.05.004]
 Dai Lianshuang,Tang Changjiang,Feng Zhizhong,et al.Risk assessment methodology and application for oil and gas pipelines’ terrorist attack[J].Oil & Gas Storage and Transportation,2011,30(09):337.[doi:10.6047/j.issn.1000-8241.2011.05.004]
[3]王乾坤,张争伟,石悦,等.埋地油气管道并行敷设技术发展现状[J].油气储运,2011,30(01):1.[doi:10.6047/j.issn.1000-8241.2011.01.001]
 Wang Qiankun,Zhang Zhengwei,Shi Yue,et al.Development status of the parallel laying technology in underground oil & gas pipelines[J].Oil & Gas Storage and Transportation,2011,30(09):1.[doi:10.6047/j.issn.1000-8241.2011.01.001]
[4]马伟平,贾子麒,赵晋云,等.美国油气管道法规和标准体系的管理模式[J].油气储运,2011,30(01):5.[doi:10.6047/j.issn.1000-8241.2011.01.002]
 Ma Weiping,Jia Ziqi,Zhao Jinyun,et al.Oil and gas pipeline eegulations and management mode of standard system in America[J].Oil & Gas Storage and Transportation,2011,30(09):5.[doi:10.6047/j.issn.1000-8241.2011.01.002]
[5]李鹤林.油气管道失效控制技术[J].油气储运,2011,30(06):401.[doi:10.6047/j.issn.1000-8241.2011.06.001]
 Li Helin.Failure control technique of oil & gas pipeline[J].Oil & Gas Storage and Transportation,2011,30(09):401.[doi:10.6047/j.issn.1000-8241.2011.06.001]
[6]荆宏远,郝建斌,陈英杰,等.管道地质灾害风险半定量评价方法与应用[J].油气储运,2011,30(07):497.[doi:10.6047/j.issn.1000-8241.2011.07.005]
 Jing Hongyuan,Hao Jianbin,Chen Yingjie,et al.Technique and application of geologic hazard risk semi-quantitative assessment of pipeline[J].Oil & Gas Storage and Transportation,2011,30(09):497.[doi:10.6047/j.issn.1000-8241.2011.07.005]
[7]陈敬和.管道外腐蚀直接评价技术[J].油气储运,2011,30(07):523.[doi:10.6047/j.issn.1000-8241.2011.07.012]
 Chen Jinghe.Direct assessment technology of pipeline external corrosion[J].Oil & Gas Storage and Transportation,2011,30(09):523.[doi:10.6047/j.issn.1000-8241.2011.07.012]
[8]吴琋瑛.光缆与油气管道同沟敷设应用实践[J].油气储运,2011,30(07):547.[doi:10.6047/j.issn.1000-8241.2011.07.021]
 Wu Xiying.Technique application of laying in one ditch for fiber cable and oil or gas pipeline[J].Oil & Gas Storage and Transportation,2011,30(09):547.[doi:10.6047/j.issn.1000-8241.2011.07.021]
[9]焦中良,李志文,李志勇,等.油气管道波动压力的雨流计数与分析[J].油气储运,2011,30(08):624.[doi:10.6047/j.issn.1000-8241.2011.08.007]
 Jiao Zhongliang,Li Zhiwen,Li Zhiyong,et al.Rain-flow counting analysis of the fluctuation pressure for oil & gas pipelines[J].Oil & Gas Storage and Transportation,2011,30(09):624.[doi:10.6047/j.issn.1000-8241.2011.08.007]
[10]樊文斌,罗自治,张策.管内高压封堵器的研制[J].油气储运,2011,30(08):657.[doi:10.6047/j.issn.1000-8241.2011.08.015]
 Fan Wenbin,Luo Zizhi,Zhang Ce.Development of high-pressure pipeline isolation plug[J].Oil & Gas Storage and Transportation,2011,30(09):657.[doi:10.6047/j.issn.1000-8241.2011.08.015]

备注/Memo

(收稿日期:2018-03-30;修回日期:2020-05-22;编辑:杜娟)
基金项目:四川省重点研发项目“含点蚀缺陷油气输送管道安全 裕度与剩余寿命在线监测平台”,017GZ0423。
作者简介:江怡舟,男,1995 年生,在读硕士生,2017 年毕业于 四川大学机械设计制造及自动化专业,现主要从事管道腐蚀、图 像处理等方向的研究工作。地址:四川省成都市武侯区一环路南 一段24 号四川大学制造科学与工程学院226 室,610065。电话: 15882613670。Email:985046984@qq.com

更新日期/Last Update: 2020-09-25