[1]许爱华,张靖,院振刚,等.新疆克深2气田双金属复合管失效原因[J].油气储运,2014,33(9):1024-1028.[doi:10.6047/j.issn.1000-8241.2014.09.024]
 XU Aihua,ZHANG Jing,YUAN Zhengang,et al.Failure cause of bi-metal composite pipe of Xinjiang No.2 Keshen Gasfield[J].Oil & Gas Storage and Transportation,2014,33(9):1024-1028.[doi:10.6047/j.issn.1000-8241.2014.09.024]
点击复制

新疆克深2气田双金属复合管失效原因

参考文献/References:

[1]朱洪亮. 克深 2 气田用双金属复合管焊接工艺评定报告[R]. 成都:四川石油天然气建设工程有限责任公司工程技术开发培训中心, 2012.

 ZHU H L.KE S. Evaluation report of bimetal clad pipe welding technology in gas field[R].Chengdu:Engineering technology development training center, SPC, 2012.

[2]刘勇,候远盛,王义,等. 双金属复合管道在牙哈凝析气田的应用[J].油气田地面工程, 2006, 25 (9): 1-2.

 LIU Y,HOU Y S,WANG Y,et al.Application of bimetal clad pipe in YahaCondensate Field [J]. Oil-Gasfield Surface Engineering, 2006, 25 (9): 1-2.

[3]许爱华,院振刚,杨光,等.双金属复合管施工焊接技术[J].天然气与石油, 2010, 12 (6): 22-28.

 XU A H,YUAN Z G,YANG G,et al. Welding technology of bimetal clad pipe[J]. Natural Gas and Oil, 2010, 12 (6): 22-28.

[4]吕世雄,王廷,冯吉才. 20G/316L 双金属复合管弧焊接头组织与性能[J].焊接学报, 2009, 30 (4): 93-96.

 LU S X,WANG T,FENG J C. Microstructure and mechanical properties of TIG welded 20G/31 6L clad pipe joint [J]. Transactions of the China Welding Institution, 2009, 30 (4): 93-96.

[5]杨平生,俞进,柯勇,等. 双金属复合钢管界面及焊缝的微观结构[J].南昌大学学报(理科版), 2005, 29 (6): 603-609.

 YANG P S,YU J,KE Y,et al Microstructure of interface and welding seam in dual-metal clad steel pipe[J]. Journal of Nanchang University(Natural Science), 2005, 29 (6): 603-609.

[6]刘建彬,韩静涛,鲍善勤,等. 热处理对双金属复合管 X60/2205组织及力学性能的影响[J]. 热加工工艺, 2009, 38 (4): 23-26.

 LIU J B,HAN J T,BAO S Q,et al. Effect of heat treatment on microstructure and meehanical properties of bimetal clad pipe X60/2205 [J]. Hot Working Technology, 2009, 38 (4): 23-26.

相似文献/References:

[1]刘悦,孟贺学.油气管道裂纹评价方法[J].油气储运,2010,29(9):660.[doi:10.6047/j.issn.1000-8241.2010.09.005]
 Liu Yue,Meng Hexue.Crack Evaluation Method of Oil & Gas Pipelines[J].Oil & Gas Storage and Transportation,2010,29(9):660.[doi:10.6047/j.issn.1000-8241.2010.09.005]
[2]帅健,许葵.裂纹管道失效评定中的有限元方法[J].油气储运,2003,22(3):18.[doi:10.6047/j.issn.1000-8241.2003.03.005]
 SHUAI Jian,XU Kui.Finite Element Method of Failure Assessment of Cracked Pipe[J].Oil & Gas Storage and Transportation,2003,22(9):18.[doi:10.6047/j.issn.1000-8241.2003.03.005]
[3]朱春鸣,陈宏达,赵新伟,等.含360°表面裂纹管道剩余强度评价[J].油气储运,2001,20(9):41.[doi:10.6047/j.issn.1000-8241.2001.09.011]
 Zhu Chunming,Chen Hongda.The Remaining Strength Assessment of Pipeline Containing 360°Cir-cumferential Surface Crack[J].Oil & Gas Storage and Transportation,2001,20(9):41.[doi:10.6047/j.issn.1000-8241.2001.09.011]
[4]董绍华,吕英民.管道裂纹的随机有限元可靠性研究[J].油气储运,1999,18(10):21.[doi:10.6047/j.issn.1000-8241.1999.10.006]
 Dong Shaohua,LüYingmin.The Research of Reliability on the Pipeline Cracks by Stochastic Finite Element[J].Oil & Gas Storage and Transportation,1999,18(9):21.[doi:10.6047/j.issn.1000-8241.1999.10.006]
[5]吕英民,蒋云.含裂纹管道承压能力的评定[J].油气储运,1998,17(12):21.[doi:10.6047/j.issn.1000-8241.1998.12.007]
 Lu Yingmin,Jiang Yun.Evaluation to pressure bearing capability of cracked pipeline[J].Oil & Gas Storage and Transportation,1998,17(9):21.[doi:10.6047/j.issn.1000-8241.1998.12.007]
[6]冯庆善,倪敬金.裂纹内检测技术应用于管道螺旋焊缝的可行性分析[J].油气储运,2009,28(11):45.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.011]
 FENG Qingshan,NI Jingjin.Feasibility Analysis of Internal Detection Technology for Crack in Spiral Seam Pipeline[J].Oil & Gas Storage and Transportation,2009,28(9):45.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.011]
[7]薛正林,刘觉非,黄烈勇,等.管道对接环焊缝裂纹的防治措施[J].油气储运,2005,24(7):51.[doi:10.6047/j.issn.1000-8241.2005.07.015]
 XUE Zhenglin,LIU Juefei.Solution to the Cracks of Girth Welding of Pipeline[J].Oil & Gas Storage and Transportation,2005,24(9):51.[doi:10.6047/j.issn.1000-8241.2005.07.015]
[8]署恒木.薄壁管道表面裂纹的应力强度因子计算[J].油气储运,2001,20(3):25.[doi:10.6047/j.issn.1000-8241.2001.03.007]
 Shu Hengmu.Stress Intensity Factors for Surface Cracks in Thin Pipes[J].Oil & Gas Storage and Transportation,2001,20(9):25.[doi:10.6047/j.issn.1000-8241.2001.03.007]
[9]董绍华,吕英民.螺旋焊管焊缝区Ⅰ/Ⅱ型裂纹R阻力曲线的确定[J].油气储运,2000,19(5):26.[doi:DOI:10.6047/j.issn.1000-8241.2000.05.008]
 Dong Shaohua,Lv Yingmin.The Determination of R Resistance on the Ⅰ/Ⅱ Cracks of Spiral Welded Pipe in Welding Line Zone[J].Oil & Gas Storage and Transportation,2000,19(9):26.[doi:DOI:10.6047/j.issn.1000-8241.2000.05.008]
[10]谷鸣.中洛复线电动阀门壳体开裂的原因分析[J].油气储运,2000,19(9):38.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.010]
 Gu Ming.Case Analysis on Valve Casing Cracking in Zhong-Luo Parallel Oil Pipeline[J].Oil & Gas Storage and Transportation,2000,19(9):38.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.010]

备注/Memo

收稿日期:2013-8-23;改回日期:2013-8-23。
基金项目:中国石油天然气集团公司产能建设项目“克深2气田地面建设工程”,油勘字2012-117。
作者简介:许爱华,在读硕士生,工程师,1981年生,2005年毕业于吉林大学自动化专业,现主要从事油气田基本建设和工程方案设计等工作。Tel:13779689225,Email:xuaih-tlm@petrochina.com.cn

更新日期/Last Update: 1900-01-01