[1]李睿,侯宇,刘淑聪,等.锚纹特征对管道外防腐环氧涂层附着力的影响[J].油气储运,2011,30(05):355-358.[doi:10.6047/j.issn.1000-8241.2011.05.010]
 Li Rui,Hou Yu,Li Jingmiao,et al.Impact of pattern on the adhesion of pipe external epoxy coating[J].Oil & Gas Storage and Transportation,2011,30(05):355-358.[doi:10.6047/j.issn.1000-8241.2011.05.010]
点击复制

锚纹特征对管道外防腐环氧涂层附着力的影响

参考文献/References:

[1 ] 杨晖,潘少明.基体表面粗糙度对涂层结合强度的影响[J].金属铸锻焊技术,2008(8):118-121.
[2] 时秀伟,崔超.埋地管道防腐层表面处理质量的影响因素[J].涂装和电镀,2009(8):25-27.
[3 ] 郑国娟.GB/T 5210-2006 色漆和清漆拉开法附着力试验[S].北京:中国标准出版社,2007.
[4 ] 洪栋煌,刘盘兴,鲁先庚,等.GB/T 8923-2008 涂装前钢材表面锈蚀等级和除锈等级[S].北京:中国标准出版社,2008.
[5?] 张瑛,许传新,权忠舆,等.SY/T0315-2005 钢质管道单层熔结环氧粉末外涂层技术规范[S].北京:石油工业出版社,2005.
[6 ] 张振远,张子起,肖利明,等.SY/T0066-1999 钢管防腐层厚度的无损测量方法(磁性法)[S].北京:石油工业出版社,1999.
[7 ] 韩[树强,刘泽年,刘军,等.不同表面处理方法对环氧胶粘涂层剪切强度影响[J].辽宁石油化工大学学报,2009,29(3):55-57.
[8 ] 刘志文,刘敬福,李赫亮,等.表面处理对环氧胶粘涂层剪切强度的影响[J].表面技术,2002,31(3):12-13.

相似文献/References:

[1]滕延平,蔡培培,徐承伟,等.应用同步监测法定位管道杂散电流的干扰源[J].油气储运,2011,30(05):347.[doi:10.6047/j.issn.1000-8241.2011.05.007]
 Teng Yanping,Cai Peipei,Xu Chengwei,et al.Applying synchronous monitoring method to locate interference sources of stray current in pipeline[J].Oil & Gas Storage and Transportation,2011,30(05):347.[doi:10.6047/j.issn.1000-8241.2011.05.007]
[2]段纪淼,宫敬,张宇,等.多相混输管道蜡沉积研究进展[J].油气储运,2011,30(04):241.[doi:10.6047/j.issn.1000-8241.2011.04.001]
 Duan Jimiao,Gong Jing,Zhang Yu,et al.Research progress of wax deposition in multiphase mixed transmission pipeline[J].Oil & Gas Storage and Transportation,2011,30(05):241.[doi:10.6047/j.issn.1000-8241.2011.04.001]
[3]薛光,袁献忠,张继亮.基于完整性管理的川气东送数字化管道系统[J].油气储运,2011,30(04):266.[doi:10.6047/j.issn.1000-8241.2011.04.007]
 Xue Guang,Yuan Xianzhong,Zhang Jiliang.Integrity management-based digitalization system of Sichuan Gas-to-East Transmission Pipeline[J].Oil & Gas Storage and Transportation,2011,30(05):266.[doi:10.6047/j.issn.1000-8241.2011.04.007]
[4]宋晓琴,刘广文,王雯娟.管道油品泄漏原因及其对环境的影响[J].油气储运,2011,30(04):297.[doi:10.6047/j.issn.1000-8241.2011.04.016]
 Song Xiaoqin,Liu Guangwen,Wang Wenjuan. The influence of oil pipeline leakage on environmental pollution [J].Oil & Gas Storage and Transportation,2011,30(05):297.[doi:10.6047/j.issn.1000-8241.2011.04.016]
[5]蔡亮学,何利民,吕宇玲,等.水平定向钻管道穿越孔底泥浆的力学特性[J].油气储运,2011,30(01):25.[doi:10.6047/j.issn.1000-8241.2011.01.007]
 Cai Liangxue,He Limin,Lv Yuling,et al.Hole-bottom slurry mechanical properties of horizontal directional drilling in pipeline crossing project[J].Oil & Gas Storage and Transportation,2011,30(05):25.[doi:10.6047/j.issn.1000-8241.2011.01.007]
[6]彭忍社,杨鲁明,屠明刚.天然气分输站场带冷凝水管道的防腐[J].油气储运,2011,30(01):41.[doi:10.6047/j.issn.1000-8241.2011.01.011]
 Peng Renshe,Yang Luming,Tu Minggang.Corrosion control on the pipeline contained condensation water in natural gas offtake station[J].Oil & Gas Storage and Transportation,2011,30(05):41.[doi:10.6047/j.issn.1000-8241.2011.01.011]
[7]樊三新,刘玉玲,楚威威.高寒地区管道低温水试压方法[J].油气储运,2011,30(01):73.[doi:10.6047/j.issn.1000-8241.2011.01.020]
 Fan Sanxin,Liu Yuling,Chu Weiwei.Pipeline hydrotest method of cold water in frigid zone[J].Oil & Gas Storage and Transportation,2011,30(05):73.[doi:10.6047/j.issn.1000-8241.2011.01.020]
[8]杜明俊,张振庭,张朝阳,等.多相混输管道90°弯管冲蚀破坏应力分析[J].油气储运,2011,30(06):427.[doi:10.6047/j.issn.1000-8241.2011.06.006]
 Du Mingjun,Chao Ling,Fu Xiaodong,et al.Analysis of erosion fracture stress of 90° elbow in multi-phase mixed transmission pipeline[J].Oil & Gas Storage and Transportation,2011,30(05):427.[doi:10.6047/j.issn.1000-8241.2011.06.006]
[9]罗金恒,杨锋平,马秋荣,等.新建大落差管道试压排水爆管原因分析[J].油气储运,2011,30(06):441.[doi:10.6047/j.issn.1000-8241.2011.06.010]
 Luo Jinheng,Yang Fengping,Ma Qiurong,et al.Reason analysis on pipe fracture in hydrotest during water draining for a newly-built pipeline with great fall[J].Oil & Gas Storage and Transportation,2011,30(05):441.[doi:10.6047/j.issn.1000-8241.2011.06.010]
[10]高河东,祁志江,任金岭,等.川气东送管道野三河跨越方案比选与实施[J].油气储运,2011,30(06):445.[doi:10.6047/j.issn.1000-8241.2011.06.011]
 Gao Hedong,Qi Zhijiang,Ren Jinling,et al.Programs comparison and construction of the Yesanhe River Overhead Crossing NG Project of Sichuan-to-East Gas Pipeline[J].Oil & Gas Storage and Transportation,2011,30(05):445.[doi:10.6047/j.issn.1000-8241.2011.06.011]
[11]徐昌学 马厚逢.管道防腐作业工艺参数及其算法[J].油气储运,2012,31(5):379.[doi:10.6047/j.issn.1000-8241.2012.05.015]
 Xu Changxue and Ma Houfeng.Technological parameters and calculation in anti-corrosion operation of pipeline[J].Oil & Gas Storage and Transportation,2012,31(05):379.[doi:10.6047/j.issn.1000-8241.2012.05.015]
[12]乔军平,张嗣伋,张永宏,等.油气管道防腐保温一次成型新工艺[J].油气储运,2006,25(4):38.[doi:10.6047/j.issn.1000-8241.2006.04.010]
 QIAO Junping,ZHANG Siji.The Method of Once-step Moulding Used in Manufacturing of Pipeline Coating[J].Oil & Gas Storage and Transportation,2006,25(05):38.[doi:10.6047/j.issn.1000-8241.2006.04.010]
[13]葛国防.管道内涂层经济可行性分析[J].油气储运,2003,22(2):54.[doi:10.6047/j.issn.1000-8241.2003.02.014]
 GE Guofang.Economy and Feasibility Analysis on Internal Coating of Pipeline[J].Oil & Gas Storage and Transportation,2003,22(05):54.[doi:10.6047/j.issn.1000-8241.2003.02.014]
[14]何英勇,杨鼎文.管道内喷涂防腐技术的应用[J].油气储运,1999,18(4):30.[doi:10.6047/j.issn.1000-8241.1999.04.008]
 He Yingyong,Yang Dingwen.Pipeline Coating Spraying Technique[J].Oil & Gas Storage and Transportation,1999,18(05):30.[doi:10.6047/j.issn.1000-8241.1999.04.008]
[15]姜炳卫.管道塑膜管内衬施工方法[J].油气储运,1998,17(8):23.[doi:10.6047/j.issn.1000-8241.1998.08.008]
 Jiang Bingwei.Installation method of pipeline plastic film inner lining[J].Oil & Gas Storage and Transportation,1998,17(05):23.[doi:10.6047/j.issn.1000-8241.1998.08.008]
[16]尹国耀,龚胜起,卢效顺.管道三层PE防腐技术及设备[J].油气储运,1998,17(3):20.[doi:10.6047/j.issn.1000-8241.1998.03.007]
 Yin Guoyao,Gong Shengqi.Pipeline three-layer PE corrosion protection technology and equipment[J].Oil & Gas Storage and Transportation,1998,17(05):20.[doi:10.6047/j.issn.1000-8241.1998.03.007]
[17]罗富绪.环氧树脂/煤焦油瓷漆管道防腐新工艺[J].油气储运,1997,16(12):59.[doi:10.6047/j.issn.1000-8241.1997.12.018]
 Luo Fuxu.Epoxy Resin and Coal Tar Enamel Coatings Used in the Corrosion Control of Pipeline[J].Oil & Gas Storage and Transportation,1997,16(05):59.[doi:10.6047/j.issn.1000-8241.1997.12.018]
[18]马书定,王学善.管道内防腐现场双球挤涂新工艺[J].油气储运,1997,16(6):28.[doi:10.6047/j.issn.1000-8241.1997.06.009]
 Ma Shuding,Wang Xueshan.A New Process for the Application of Internal Insitu Pipeline Coating with Double-Pig[J].Oil & Gas Storage and Transportation,1997,16(05):28.[doi:10.6047/j.issn.1000-8241.1997.06.009]
[19]白淑媛.涂塑钢的耐蚀性能及其应用[J].油气储运,1997,16(2):31.[doi:10.6047/j.issn.1000-8241.1997.02.011]
 Bai Shuyuan.The Corrosion Resistance of Clad Steel and its Application[J].Oil & Gas Storage and Transportation,1997,16(05):31.[doi:10.6047/j.issn.1000-8241.1997.02.011]
[20]马书定.聚乙烯管套接衬里新工艺[J].油气储运,1996,15(12):27.[doi:10.6047/j.issn.1000-8241.1996.12.008]
 Ma Shuding.A New Technology for Liner Insertion of PE Plastic Pipe[J].Oil & Gas Storage and Transportation,1996,15(05):27.[doi:10.6047/j.issn.1000-8241.1996.12.008]

备注/Memo

李睿,助理工程师,1983 年生,2009 年硕士毕业于吉林大学精密仪器与机械设计专业,现主要从事管道防腐和节能技术的研究工作。
电话:15003162325;Email:kjlirui@petrochina.com.cn(收稿日期:2010-11-04)

更新日期/Last Update: