[1]陈建民,孟惠民,李英义.腐蚀后管道时效分析与爆破试验[J].油气储运,1998,17(3):28-30.[doi:10.6047/j.issn.1000-8241.1998.03.009]
 Chen Jianmin,Meng Huimin.Pipeline prescription analysis after corrosion and explosive test[J].Oil & Gas Storage and Transportation,1998,17(3):28-30.[doi:10.6047/j.issn.1000-8241.1998.03.009]
点击复制

腐蚀后管道时效分析与爆破试验

相似文献/References:

[1]谢文江,魏斌,陈娟利,等.含H2S/CO2气田油套管腐蚀与防护技术[J].油气储运,2010,29(2):93.[doi:10.6047/j.issn.1000-8241.2010.02.004]
 Xie Wenjiang,Wei Bin,Chen Juanli.Casing Steel Corrosion in H2S/CO2-contained Gas Field and Its Protection Technology[J].Oil & Gas Storage and Transportation,2010,29(3):93.[doi:10.6047/j.issn.1000-8241.2010.02.004]
[2]陈迪.塔河油田原油集输管道弯管开裂原因[J].油气储运,2011,30(05):396.[doi:10.6047/j.issn.1000-8241.2011.05.021]
 Chen Di.Bended pipe cracking reason of gathering pipeline in Tahe Oilfield[J].Oil & Gas Storage and Transportation,2011,30(3):396.[doi:10.6047/j.issn.1000-8241.2011.05.021]
[3]王霞,白媛丽.特稠油降粘剂筛选及其缓蚀效果评价[J].油气储运,2011,30(03):177.[doi:10.6047/j.issn.1000-8241.2011.03.005]
 Wang Xia and Bai Yuanli.Selection on viscosity reducer for extra-heavy oil and corrosion inhibition effectiveness evaluation [J].Oil & Gas Storage and Transportation,2011,30(3):177.[doi:10.6047/j.issn.1000-8241.2011.03.005]
[4]胡士信,陆家榆,张本革,等.邻近强电线路管道交流干扰参数的测试方法[J].油气储运,2011,30(03):203.[doi:10.6047/j.issn.1000-8241.2011.03.012]
 Hu Shixin,Lu Jiayu,Zhang Benge,et al.Test method of AC interference parameters for pipeline adjacent power transmission lines[J].Oil & Gas Storage and Transportation,2011,30(3):203.[doi:10.6047/j.issn.1000-8241.2011.03.012]
[5]张贵喜,唐和清,金鑫,等.高压输电线路对埋地钢质管道的腐蚀影响[J].油气储运,2011,30(02):125.[doi:10.6047/j.issn.1000-8241.2011.02.012]
 Zhang Guixi,Tang Heqing,Jin Xin,et al.Effects of high-voltage power line on corrosion of buried steel pipeline[J].Oil & Gas Storage and Transportation,2011,30(3):125.[doi:10.6047/j.issn.1000-8241.2011.02.012]
[6]康叶伟,林明春,王维斌,等.罐底板声发射在线检测影响因素与评价可靠性[J].油气储运,2011,30(05):343.[doi:10.6047/j.issn.1000-8241.2011.05.006]
 Kang Yewei,Lin Mingchun,Wang Weibin,et al.Influencing factors of acoustic emission technique and evaluation reliability in inspection of tank floor[J].Oil & Gas Storage and Transportation,2011,30(3):343.[doi:10.6047/j.issn.1000-8241.2011.05.006]
[7]叶帆,杨伟.塔河油田集输管道腐蚀与防腐技术[J].油气储运,2010,29(5):354.[doi:10.6047/j.issn.1000-8241.2010.05.011]
 Ye Fan and Yang Wei.Corrosion and Corrosion Control of Gathering Pipelines in Tahe Oilfield[J].Oil & Gas Storage and Transportation,2010,29(3):354.[doi:10.6047/j.issn.1000-8241.2010.05.011]
[8]李铁明,王志彬,石红艳.氢致微裂纹应力腐蚀损伤管道的寿命预测[J].油气储运,2011,30(08):637.[doi:10.6047/j.issn.1000-8241.2011.08.010]
 Li Tieming,Wang Zhibin,Shi Hongyan.Service life prediction of pipeline under hydrogen-induced microcrack stress corrosion[J].Oil & Gas Storage and Transportation,2011,30(3):637.[doi:10.6047/j.issn.1000-8241.2011.08.010]
[9]石鑫,张志宏,刘强,等.塔河某单井管道频繁穿孔原因[J].油气储运,2011,30(11):848.[doi:10.6047/j.issn.1000-8241.2011.11.014]
 Shi Xin,Zhang Zhihong,Liu Qiang,et al.Reason analysis on the corrosion to leak pipeline of well[J].Oil & Gas Storage and Transportation,2011,30(3):848.[doi:10.6047/j.issn.1000-8241.2011.11.014]
[10]郑云萍,舒洁,李蕾,等.陆梁油田生产系统腐蚀影响因素的灰关联分析[J].油气储运,2010,29(10):774.[doi:10.6047/j.issn.1000-8241.2010.10.015]
 Zheng Yunping,Shu Jie,Li Lei.Grey Relational Analysis on Influence Factors of Corrosion in Production System of Luliang Oilfield[J].Oil & Gas Storage and Transportation,2010,29(3):774.[doi:10.6047/j.issn.1000-8241.2010.10.015]

备注/Memo

收稿日期:1997-8-25。
作者简介:陈建民,工程师,1957年生,1985年毕业于原中国石油天然气管道职工学院线路工程专业,现在中国石油天然气华东输油管理局储运部从事管道管理工作.

更新日期/Last Update: 1900-01-01