[1]常香荣,朱淑彦,董义娟.石油管线用钢材的转变温度[J].油气储运,1988,7(4):38-42.[doi:DOI:10.6047/j.issn.1000-8241.1988.04.011]
 Chang Xiangrong.The Transition Temperature of the Steel for Oil Pipelines[J].Oil & Gas Storage and Transportation,1988,7(4):38-42.[doi:DOI:10.6047/j.issn.1000-8241.1988.04.011]
点击复制

石油管线用钢材的转变温度

参考文献/References:

[1] W.A.Maxey et al: Fracture Toughness, ASTM STP, 514 (1972), P79
[2] R.J.Podlasek et al: J.of eng.Mates and Tech, 1974, P330
[3] R.J.Eiber et al: The Oil and Gas J, (1963) Sept.23, P158
[4] API Spee 5 LS, 1980
[5] API RP 5 L3

相似文献/References:

[1]尹国耀.包申格效应对X65管道钢管强度的影响[J].油气储运,2002,21(12):43.[doi:10.6047/j.issn.1000-8241.2002.12.012]
 YIN Guoyao.The Influence of Bauschinger Effect upon the Strength of X65 Pipe Steel[J].Oil & Gas Storage and Transportation,2002,21(4):43.[doi:10.6047/j.issn.1000-8241.2002.12.012]
[2]马秋荣,霍春勇,冯耀荣.国外X80管道钢管的研究与应用现状[J].油气储运,2000,19(11):9.[doi:DOI:10.6047/j.issn.1000-8241.2000.11.003]
 Ma Qiurong,Huo Chunyong.The Development and Application Actualites of Oversea XSO Line Pipe[J].Oil & Gas Storage and Transportation,2000,19(4):9.[doi:DOI:10.6047/j.issn.1000-8241.2000.11.003]
[3]牛辉.钢管生产管端涂敷煤焦油瓷漆覆盖层技术[J].油气储运,1998,17(7):36.[doi:10.6047/j.issn.1000-8241.1998.07.011]
 Niu Hui.Coal tar enamel coating technology on pipe end in steel pipe’s production[J].Oil & Gas Storage and Transportation,1998,17(4):36.[doi:10.6047/j.issn.1000-8241.1998.07.011]
[4]陈建民,孟惠民,李英义.腐蚀后管道时效分析与爆破试验[J].油气储运,1998,17(3):28.[doi:10.6047/j.issn.1000-8241.1998.03.009]
 Chen Jianmin,Meng Huimin.Pipeline prescription analysis after corrosion and explosive test[J].Oil & Gas Storage and Transportation,1998,17(4):28.[doi:10.6047/j.issn.1000-8241.1998.03.009]
[5]潘家华.关于输气管道氢致裂纹的研究[J].油气储运,1997,16(12):1.[doi:DOI:10.6047/j.issn.1000-8241.1997.12.001]
 Pan Jiahua.An Approach to the SCC of Gas Transmission Pipeline[J].Oil & Gas Storage and Transportation,1997,16(4):1.[doi:DOI:10.6047/j.issn.1000-8241.1997.12.001]
[6]孙德佑,何洪勇.长江跨越工程的主管管材抗裂性能试验[J].油气储运,1991,10(2):38.[doi:10.6047/j.issn.1000-8241.1991.02.009]
[7]靳东来,赵跃曾,张春蕴,等.全尺寸管道的爆破试验及转变温度[J].油气储运,1988,7(4):33.[doi:DOI:10.6047/j.issn.1000-8241.1988.04.010]
 Jin Donglai.Explosion Test of a Whole Scaled Pipeline and the Trastion Temperature[J].Oil & Gas Storage and Transportation,1988,7(4):33.[doi:DOI:10.6047/j.issn.1000-8241.1988.04.010]
[8]牛吉录,陈安利,赫飚,等.X70钢管全位置自动焊的试验分析[J].油气储运,2001,20(7):57.[doi:DOI:10.6047/j.issn.1000-8241.2001.07.016]
 Niu Jilu,Chen Anli.Experiment on All Position Automatic Welding for X70 Steel Pipe[J].Oil & Gas Storage and Transportation,2001,20(4):57.[doi:DOI:10.6047/j.issn.1000-8241.2001.07.016]
[9]尹国耀,屈涛,李光新.高强度管道钢的力学性能与分析[J].油气储运,2000,19(9):9.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.003]
 Yin Guoyao,Qu Tao.Property Analysis on High Strength Pipeline Steels[J].Oil & Gas Storage and Transportation,2000,19(4):9.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.003]
[10]王茂棠,马彦昌.油气干线用钢管质量指标确定方法[J].油气储运,1997,16(10):6.[doi:10.6047/j.issn.1000-8241.1997.10.002]
 Wang Maotang,Ma Yanchang.A Method to Determine the Quality Specifications of Oil and Gas Line Pipes[J].Oil & Gas Storage and Transportation,1997,16(4):6.[doi:10.6047/j.issn.1000-8241.1997.10.002]

备注/Memo

收稿日期:1988-3-8。

更新日期/Last Update: 1900-01-01