考虑裂纹的CNG地下储气井剩余强度数值模拟
Numerical simulation of residual strength of CNG underground gas storage well considering cracks
由于天然气中存在的硫化氢等气体具有腐蚀性,因此储气井在建设和服役过程中,井管内表面容易在腐蚀和应力的双重作用下产生裂纹,最终导致井管破裂失效。建立储气井井管-水泥环-地层数值模型,采用传统基于工作应力的方法和基于断裂力学应力强度因子的方法分析了含裂纹储气井的剩余强度,得出不同条件下许可裂纹的尺寸。结果表明,基于断裂力学应力强度因子的分析方法可以更准确地判定危险点位置,能够有效排除CNG储气井安全事故隐患。
[1]刘悦,孟贺学.油气管道裂纹评价方法[J].油气储运,2010,29(9):660.[doi:10.6047/j.issn.1000-8241.2010.09.005]
Liu Yue,Meng Hexue.Crack Evaluation Method of Oil & Gas Pipelines[J].Oil & Gas Storage and Transportation,2010,29(01):660.[doi:10.6047/j.issn.1000-8241.2010.09.005]
[2]帅健,许葵.裂纹管道失效评定中的有限元方法[J].油气储运,2003,22(3):18.[doi:10.6047/j.issn.1000-8241.2003.03.005]
SHUAI Jian,XU Kui.Finite Element Method of Failure Assessment of Cracked Pipe[J].Oil & Gas Storage and Transportation,2003,22(01):18.[doi:10.6047/j.issn.1000-8241.2003.03.005]
[3]朱春鸣,陈宏达,赵新伟,等.含360°表面裂纹管道剩余强度评价[J].油气储运,2001,20(9):41.[doi:10.6047/j.issn.1000-8241.2001.09.011]
Zhu Chunming,Chen Hongda.The Remaining Strength Assessment of Pipeline Containing 360°Cir-cumferential Surface Crack[J].Oil & Gas Storage and Transportation,2001,20(01):41.[doi:10.6047/j.issn.1000-8241.2001.09.011]
[4]董绍华,吕英民.管道裂纹的随机有限元可靠性研究[J].油气储运,1999,18(10):21.[doi:10.6047/j.issn.1000-8241.1999.10.006]
Dong Shaohua,LüYingmin.The Research of Reliability on the Pipeline Cracks by Stochastic Finite Element[J].Oil & Gas Storage and Transportation,1999,18(01):21.[doi:10.6047/j.issn.1000-8241.1999.10.006]
[5]吕英民,蒋云.含裂纹管道承压能力的评定[J].油气储运,1998,17(12):21.[doi:10.6047/j.issn.1000-8241.1998.12.007]
Lu Yingmin,Jiang Yun.Evaluation to pressure bearing capability of cracked pipeline[J].Oil & Gas Storage and Transportation,1998,17(01):21.[doi:10.6047/j.issn.1000-8241.1998.12.007]
[6]冯庆善,倪敬金.裂纹内检测技术应用于管道螺旋焊缝的可行性分析[J].油气储运,2009,28(11):45.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.011]
FENG Qingshan,NI Jingjin.Feasibility Analysis of Internal Detection Technology for Crack in Spiral Seam Pipeline[J].Oil & Gas Storage and Transportation,2009,28(01):45.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.011]
[7]薛正林,刘觉非,黄烈勇,等.管道对接环焊缝裂纹的防治措施[J].油气储运,2005,24(7):51.[doi:10.6047/j.issn.1000-8241.2005.07.015]
XUE Zhenglin,LIU Juefei.Solution to the Cracks of Girth Welding of Pipeline[J].Oil & Gas Storage and Transportation,2005,24(01):51.[doi:10.6047/j.issn.1000-8241.2005.07.015]
[8]署恒木.薄壁管道表面裂纹的应力强度因子计算[J].油气储运,2001,20(3):25.[doi:10.6047/j.issn.1000-8241.2001.03.007]
Shu Hengmu.Stress Intensity Factors for Surface Cracks in Thin Pipes[J].Oil & Gas Storage and Transportation,2001,20(01):25.[doi:10.6047/j.issn.1000-8241.2001.03.007]
[9]董绍华,吕英民.螺旋焊管焊缝区Ⅰ/Ⅱ型裂纹R阻力曲线的确定[J].油气储运,2000,19(5):26.[doi:DOI:10.6047/j.issn.1000-8241.2000.05.008]
Dong Shaohua,Lv Yingmin.The Determination of R Resistance on the Ⅰ/Ⅱ Cracks of Spiral Welded Pipe in Welding Line Zone[J].Oil & Gas Storage and Transportation,2000,19(01):26.[doi:DOI:10.6047/j.issn.1000-8241.2000.05.008]
[10]谷鸣.中洛复线电动阀门壳体开裂的原因分析[J].油气储运,2000,19(9):38.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.010]
Gu Ming.Case Analysis on Valve Casing Cracking in Zhong-Luo Parallel Oil Pipeline[J].Oil & Gas Storage and Transportation,2000,19(01):38.[doi:DOI:10.6047/j.issn.1000-8241.2000.09.010]