分享
[1]赵兴民,高睿,高晓蓓.无配重层海底管道外防腐补口工艺方案[J].油气储运,2019,38(03):356-360.[doi:10.6047/j.issn.1000-8241.2019.03.019]
 ZHAO Xingmin,GAO Rui,GAO Xiaobei.A joint coating process scheme for submarine pipelines without weight coating[J].Oil & Gas Storage and Transportation,2019,38(03):356-360.[doi:10.6047/j.issn.1000-8241.2019.03.019]
点击复制

无配重层海底管道外防腐补口工艺方案

参考文献/References:

[1] 陈新.舟山市岛北污水处理工程排海管道的设计与施工 [J].中国市政工程,2013(3):32-35.
CHEN X.Design and construction of submarine pipeline of Zhoushan North Island sewage treatment project[J].China Municipal Engineering,2013(3):32-35.
[2] 夏贤行,邵伟才.舟山大陆饮水海底管道施工技术概论[J].水利水电技术,2004,35(9):77-80.
XIA X H,SHAO W C.General description of construction technology for the continent to Zhoushan submarine water diversion pipeline[J].Water Resources and Hydropower Engineering,2004,35(9):77-80.
[3] PARIS P C,ERDOGAN F.A critical analysis of crack propagation laws[J].Journal of Basic Engineering,1963,85(4): 528-533.
[4] 刘有利,熊睿,袁举洋,等.新型补口工艺在海底管道铺设中的应用[J].海洋工程装备与技术,2017,4(3):168-172.
LIU Y L,XIONG R,YUAN J Y,et al.Application of new field joint coating process to subsea pipeline laying[J].Ocean Engineering Equipment and Technology,2017,4(3): 168-172.
[5] ROCHE M.Marcel ISO’s standard for field joint coating: understanding and using ISO 21809-3[J].Journal of Protective Coatings Linings,2012,29(7):20-29.
[6] MEGHAN M,MARIO P.A new three-layer polypropylene offshore field-joint coating[J].NACE International,2010, 49(10):36-41.
[7] 魏伟荣,郑国良 .海底管道外防腐涂层设计及涂敷工艺探讨 [J].材料开发与应用,2013,28(2):30-33.
WEI W R,ZHENG G L.Design of external anticorrosion coating and the coating process for submarine pipeline[J].Development and Application of Materials,2013,28(2):30-33.
[8] 那骥宇,赫连建峰,李爱贵,等.管道外防腐补口技术发展和趋势[J].石油工程建设,2017,43(2):1-4.
NA J Y,HELIAN J F,LI A G,et al.Discussion on development of field joint coatings for pipelines[J].Petroleum Engineering Construction,2017,43(2):1-4.
[9] 赵利,武占文,相政乐,等.海底管道节点防腐涂层结构发展概况[J].石油工程建设,2016,42(1):7-9.
ZHAO L,WU Z W,XIANG Z L,et al.Review on development of field joint coating structure for offshore pipelines[J].Petroleum Engineering Construction,2016,42(1):7-9.
[10] 宋飞,潘红丽.管道防腐补口材料及施工技术现状及展望[J].新疆石油科技,2016,26(1):46-51.
SONG F,PAN H L.Construction technology situation and prospect of pipeline antiseptic fillings[J].Xinjiang Petroleum Science and Technology,2016,26(1):46-51.
[11] 叶春艳,董彬,张鹏,等.热收缩带干、湿膜安装工艺研究[J].腐蚀科学与防护技术,2012,24(3):263-264.
YE C Y,DONG B,ZHANG P,et al.Installation technology research of dry film and wet film of heat-shrinkable tape[J].Corrosion Science and Protection Technology,2012,24(3): 263-264.
[12] 李依璇.干膜法管道外防腐热收缩补口技术的特点和优势分析[J].全面腐蚀控制,2010,24(11):21-23.
LI Y X.Characteristics and advantages analysis on dry-coating heat shrinkable sealing techniques used for pipelines[J].Total Corrosion Control,2010,24(11):21-23.
[13] 梁建国,陈国顺.干膜法补口工艺在兰郑长成品油管道工程中的应用[J].石油工程建设,2009,35(1):36-39.
LIANG J G,CHEN G S.Application of dry film approach to anticorrosion field joint in Lan-Zheng-Chang Product Pipeline[J].Petroleum Engineering Construction,2009,35(1): 36-39.
[14] 孙成赞,王允.OFFPIPE软件在海底管道铺设中的应用[J].石油工程建设,2005,31(5):49-52.
SUN C Z,WANG Y.Application of OFFPIPE software in submarine pipeline laying[J].Petroleum Engineering Construction,2005,31(5):49-52.
[15] 张韵韵,王学军.OFFPIPE在铺管计算中的应用[J].中国海洋平台,2014,29(5):52-56.
ZHANG Y Y,WANG X J.Application of OFFPIPE in pipeline laying calculation[J].China Offshore Platform,2014, 29(5):52-56.
[16] 郭艳林,梁政.海底管道铺设施工设计分析[J].石油学报, 1999,20(4):83-87.
GUO Y L,LIANG Z.Design and analysis of laying for submarine pipeline[J].Acta Petrolei Sinica,1999,20(4):83-87.
[17] 曹晓辉,柳春图,邢静中.海底管道铺设的力学分析[J].力学与实践,2002,24(4):19-21.
CAO X H,LIU C T,XING J Z.Mechanical analysis of pipe laying[J].Mechanics in Engineering,2002,24(4):19-21.
[18] 王帅.基于 J形铺管法局部屈曲校核及敏感性分析[J].石油机械,2018,46(5):39-46.
WANG S.Localbuckling check and sensitivity analysis based on J-lay[J].China Petroleum Machinery,2018,46(5):39-46.
[19] 任立元,翁乐宁,孟庆丽.管道三层热收缩套(带)现场补口应注意的问题[J].材料保护,2005,3(10):58-71.
REN L Y,WENG L N,MENG Q L.Issues related to field coating joint of heat shrinking sleeve of three-layer polyethylene pipelines[J].Materials Protection,2005,3(10):58-71.
[20] 叶春艳,张鹏,康景波,等.热收缩带中频加热补口施工技术[J].石油工程建设,2012,38(5):49-50.
YE C Y, ZHANG P,KANG J B,et al.Construction technique of field joint applying heat shrinkable tapes by intermediate frequency heating[J].Petroleum Engineering Construction, 2012,38(5):49-50.
[21] 王林章.中频感应加热在管道外补口中的应用[J].石油工程建设,1987,13(1):21-22.
WANG L Z.Electric induction heating of pipe joint coating[J].Petroleum Engineering Construction,1987,13(1):21-22.
[22] 孙海明,刘立群,张海雷.管道 3LPE防腐蚀层补口失效原因及建议[J].腐蚀与防护,2016,37(1):60-63.
SUN H M,LIU L Q,ZHANG H L.Failure reason and suggestion for 3LPE pipeline ?led joint coating[J].Corrosion & Protection,2016,37(1):60-63.

相似文献/References:

[1]张伟,杨新明.浅水海底混输管道设计压力的确定方法[J].油气储运,2011,30(01):34.[doi:10.6047/j.issn.1000-8241.2011.01.009]
 Zhang Wei and Yang Xinming.Determination method for the design pressure of offshore multiphase pipeline[J].Oil & Gas Storage and Transportation,2011,30(03):34.[doi:10.6047/j.issn.1000-8241.2011.01.009]
[2]党学博.海底管道腐蚀与剩余寿命的灰色预测[J].油气储运,2011,30(07):486.[doi:10.6047/j.issn.1000-8241.2011.07.002]
 Dang Xuebo.Prediction of corrosion and residual life of submarine pipeline with grey theory[J].Oil & Gas Storage and Transportation,2011,30(03):486.[doi:10.6047/j.issn.1000-8241.2011.07.002]
[3]谢丽婉,陈国明,鞠少栋.信息不完全时的海底管道安全评价方法[J].油气储运,2011,30(07):508.[doi:10.6047/j.issn.1000-8241.2011.07.008]
 Xie Liwan,Chen Guoming,Ju Shaodong.A method for submarine pipeline safety assessment under the incomplete information condition[J].Oil & Gas Storage and Transportation,2011,30(03):508.[doi:10.6047/j.issn.1000-8241.2011.07.008]
[4]曾春雷,于达,赵文婷,等.苏丹3/7 区海底装船原油管道的结蜡规律[J].油气储运,2011,30(09):654.[doi:10.6047/j.issn.1000-8241.2011.09.003]
 Zeng Chunlei,Yu Da,Zhao Wenting,et al.Wax deposition law of seabed shipment crude oil pipeline in Sudan 3/7 Block[J].Oil & Gas Storage and Transportation,2011,30(03):654.[doi:10.6047/j.issn.1000-8241.2011.09.003]
[5]黄俊,何绍礼,贾旭.海底管道可双向通球水下三通的设计与安装[J].油气储运,2011,30(09):705.[doi:10.6047/j.issn.1000-8241.2011.09.017]
 Huang Jun,He Shaoli,Jia Xu.Design and installation of underwater tee joint of bi-directional pig for submarine pipelines[J].Oil & Gas Storage and Transportation,2011,30(03):705.[doi:10.6047/j.issn.1000-8241.2011.09.017]
[6]张积乐,唐友刚,邵卫东,等.基于ANSYS 二次开发的海管浮拖法强度分析程序[J].油气储运,2011,30(10):750.[doi:10.6047/j.issn.1000-8241.2011.10.009]
 Zhang Jile,Tang Yougang,Shao Weidong,et al.Intensity analysis program of pipeline floating pulling method for submarine pipeline based on secondary developmentof ANSYS[J].Oil & Gas Storage and Transportation,2011,30(03):750.[doi:10.6047/j.issn.1000-8241.2011.10.009]
[7]孔芋丁,邓道明,姜念琛,等.纵向尺寸对自由站立式立管系统不稳定流动特性的影响[J].油气储运,2011,30(12):907.[doi:10.6047/j.issn.1000-8241.2011.12.008]
 Kong Yuding,Deng Daoming,Jiang Nianchen,et al.Effects of longitudinal dimensions on the unstable flow characteristics of free standing type riser system[J].Oil & Gas Storage and Transportation,2011,30(03):907.[doi:10.6047/j.issn.1000-8241.2011.12.008]
[8]王诗鹏.海底管道腐蚀缺陷修复评估方案的确定[J].油气储运,2011,30(12):949.[doi:10.6047/j.issn.1000-8241.2011.12.018]
 Wang Shipeng.Repairing corrosion defects of subsea pipe and the availability of repair method[J].Oil & Gas Storage and Transportation,2011,30(03):949.[doi:10.6047/j.issn.1000-8241.2011.12.018]
[9]严密林,梅奇,冯耀荣,等.带配重海管内壁和管端的特殊防腐技术[J].油气储运,2010,29(9):677.[doi:10.6047/j.issn.1000-8241.2010.09.010]
 Yan Milin,Mei Qi,Feng Yaorong.Special Corrosion Control Technique for Internal Pipe Wall and Pipe Ends of Submarine Pipeline with Concrete Blocks[J].Oil & Gas Storage and Transportation,2010,29(03):677.[doi:10.6047/j.issn.1000-8241.2010.09.010]
[10]余红伟,倪友伟,姚士洪.胍胶隔离技术在海底输油管道上的应用[J].油气储运,2009,28(11):75.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.022]
 YU Hongwei,NI Youwei.Application of Guargum Separation Repair Technique in Submarine Oil Pipeline[J].Oil & Gas Storage and Transportation,2009,28(03):75.[doi:DOI:10.6047/j.issn.1000-8241.2009.11.022]

备注/Memo

作者简介:赵兴民,男,1983年生,工程师, 2012年硕士毕业于东北石油大学油气储运工程专业,现主要从事海洋工程建设工作。地址:天津市经济技术开发区北塘企业总部西区 6号楼, 300457。电话:18222266234。Email:315478331@qq.com

更新日期/Last Update: 2019-03-20