[1]张振永,张文伟,周亚薇,等.中俄东线OD 1 422 mm 埋地管道的断裂控制设计[J].油气储运,2017,36(9):1059-1064.[doi:10.6047/j.issn.1000-8241.2017.09.013]
 ZHANG Zhenyong,ZHANG Wenwei,ZHOU Yawei,et al.The fracture control design of the OD 1 422 mm buried pipeline in China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(9):1059-1064.[doi:10.6047/j.issn.1000-8241.2017.09.013]
点击复制

中俄东线OD 1 422 mm 埋地管道的断裂控制设计

参考文献/References:

[1] 王旭. 油气管道断裂扩展及止裂技术研究[J]. 当代化工,2016, 45(2):331-335.
WANG X. The technology status of fracture propagation and crack arrest of pipelines[J]. Contemporary Chemical Industry, 2016,45(2):331-335.
[2] 李红克,张彦华. 天然气管道延性断裂止裂控制技术进展[J]. 石 油工程建设,2003,29(4):1-5.
LI H K,ZHANG Y H. The development of ductile fracture arrest control technique in natural gas pipelines[J]. Petroleum Engineering Construction,2003,29(4):1-5.
[3] 潘家华. 关于西气东输工程中管道止裂问题的思考[J]. 油气储 运,2001,20(4):41-46.
PAN J H. Thinking on fracture arrest of pipeline in West-East Pipeline Project[J]. Oil & Gas Storage and Transporation,2001, 20(4):41-46.
[4] 陈福来,帅健,祝宝利. 高钢级输气管线钢的止裂设计判据研 究[J]. 压力容器,2010,27(8):81-85.
CHEN F L,SHUAI J,ZHU B L. Studies on crack arrest criterion of high-grade gas transmission pipeline steel[J]. Pressure Vessel Technology,2010,27(8):81-85.
[5] 宫敬,邱伟伟,赵建奎. 输气管道断裂过程中减压波传播特性研 究[J]. 天然气工业,2010,30(11):130-135.
GONG J,QIU W W,ZHAO J K. Propagation characteristics of decompression wave in the gas transmission pipeline fracture process[J]. Natural Gas Industry,2010,30(11):130-135.
[6] American Petroleum Institute. Specification for 1ine pipe:API SPEC 5L-2009[S]. Washington D C:API Publishing Services, 2012:36-38.
[7] ANDREWS R M,CUMBER P S,LIU J H. Revision of the BG (British Gas)model for ductile shear fracture in gas transmission pipelines[J]. Pipeline Technology,2000(1):421-436.
[8] 杨政,冯耀荣,陈宏达,等. 高性能管线钢DWTT 试样异常断口 分析[J]. 焊管,2006,29(4):25-30.
YANG Z,FENG Y R,CHEN H D,et al. Analysis on abnormal fracture of DWTT specimen for pipeline steel with high property[J]. Weld Pipe and Tube,2006,29(4):25-30.
[9] LEIS B N,EIBER R J,CARLSON R J,et al. Relationship between apparent(total) charpy vee-notch toughness and the corresponding dynamic crack-propagation resistance[C]. Calgary: International Pipeline Conference,1998:723-731.
[10] EIBER R J. Fracture control technology for natural gas pipelines[R]. Houston:Technical Toolboxes Inc.,1993: 94015614.
[11] CUNHA S B. Comparison and analysis of pipeline failure statistics[C]. Calgary:Proceedings of the 9th International Pipeline Conference,2012:IPC2012-90186.
[12] 霍春勇,李鹤,张伟卫,等. X80 钢级1 422 mm 大口径管道断 裂控制技术[J]. 天然气工业,2016,36(6):78-83.
HUO C Y,LI H,ZHANG W W,et al. Fracture control technology for the X80 large OD 1422 mm line pipes[J].Natural Gas Industry,2016,36(6):78-83.
[13] 王仪康,杨柯,单以银,等. 高压输气管线用钢[J]. 焊管,2002, 25(1):1-10.
WANG Y K,YANG K,SHAN Y Y,et al. High pressure gas transmitting pipeline steel[J]. Weld Pipe and Tube,2002, 25(1):1-10.
[14] 高惠临. 管线钢管韧性的设计和预测[J]. 焊管,2010,33(12): 5-12.
GAO H L. The design and prediction of linepipe toughness[J].Weld Pipe and Tube,2010,33(12):5-12.
[15] 霍春勇,李鹤林. 西气东输二线延性断裂与止裂研究[J]. 金属 热处理,2011,36(增刊1):4-9.
HUO C Y,LI H L. Ductile fracture arrest toughness of 2nd West-East Gas PipeIine[J]. Heat Treatment of Metals,2011, 36(S1):4-9.
[16] MAKINO H,KUBO T,SHIWAKU T,et al. Prediction for crack propagation and arrest of shear fracture in ultra high pressure natural gas pipelines[J]. Transactions of the Iron & Steel Institute of Japan,200l,41(4):381-388.
[17] RUDINGER G. Wave digram for nonsteady flow in ducts[M].New York:D Van Nonstrand Company Inc.,1955:55-70.
[18] 张伟卫,李鹤,池强. 外径1 422 mm 的X80 钢级管材技术条件 研究及产品开发[J]. 天然气工业,2016,36(6):84-91.
ZHANG W W,LI H,CHI Q. Technical specifications of the X80 large OD 1 422 mm line pipes and the corresponding product development[J]. Natural Gas Industry,2016,36(6):84-91.
[19] 田野. 长输油气管道环焊缝缺陷评价的研究[J]. 内蒙古石油化 工,2013(19):12-14.
TIAN Y. Long-distance oil and gas pipeline girth weld evaluation studies[J]. Inner Mongolia Petrochemical Industry, 2013(19):12-14.
[20] 王卫东. 焊接缺陷对管道安全可靠性影响分析[J]. 焊管,2007, 30(2):27-29.
WANG W D. Analysis of the influence of welding defects on pipeline safety reliability[J]. Welded Pipe and Tube,2007, 30(2):27-29

相似文献/References:

[1]赵国辉.长输油气管道自控技术的发展与中俄东线SCADA系统[J].油气储运,2020,39(01):1.
 ZHAO Guohui.Development of long-distance oil and gas pipeline automatic control technology and SCADA system for China–Russia Eastern Gas Pipeline [J].Oil & Gas Storage and Transportation,2020,39(9):1.
[2]闫锋,欧阳欣,王鹏宇,等.输气管道干线强度设计原则[J].油气储运,2016,35(10):1112.[doi:10.6047/j.issn.1000-8241.2016.10.016]
 YAN Feng,OUYANG Xin,WANG Pengyu,et al.Strength design principles for main gas pipelines[J].Oil & Gas Storage and Transportation,2016,35(9):1112.[doi:10.6047/j.issn.1000-8241.2016.10.016]
[3]周亚薇 张振永.中俄东线天然气管道环焊缝断裂韧性设计[J].油气储运,2018,37(预出版):1.
 ZHOU Yawei,ZHANG Zhenyong.The design for the fracture toughness of girth weld in Russia-China Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2018,37(9):1.
[4]张振永 周亚薇 张金源.现行设计系数对中俄东线OD 1 422 mm 管道的适用性[J].油气储运,2017,36(预出版):1.
 ZHANG Zhenyong,ZHOU Yawei,ZHANG Jinyuan.Applicability of current design coefficient to OD 1 422mm pipelines in China-Russia East Natural Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(9):1.
[5]王巨洪 姜有文 滕延平.中俄东线阴极保护远程监控系统的建设实践[J].油气储运,2020,39(01):1.
 WANG Juhong,JIANG Youwen,TENG Yanping.Construction practice of remote monitoring system for cathodic protection in China–Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2020,39(9):1.
[6]刘阳 李雨佳 牛亚琨 王天祺.中俄东线无损检测技术及AUT质量控制体系[J].油气储运,2020,39(中俄东线):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
 LIU Yang,LI Yujia,NIU Yakun,et al.NDT technology and AUT quality control system applied in China-Russia Eastern Gas Pipeline Project[J].Oil & Gas Storage and Transportation,2020,39(9):1.[doi:10.6047/j.issn.1000-8241.2020.00.000]
[7]张振永,周亚薇,张金源.现行设计系数对中俄东线OD 1 422 mm 管道的适用性[J].油气储运,2017,36(3):319.[doi:10.6047/j.issn.1000-8241.2017.03.014]
 ZHANG Zhenyong,ZHOU Yawei,ZHANG Jinyuan.Applicability of current design coefficient to OD 1 422 mm pipelines in China-Russia East Natural Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(9):319.[doi:10.6047/j.issn.1000-8241.2017.03.014]
[8]张振永 张文伟 周亚薇 薄国公.中俄东线OD 1 422 mm 埋地管道的断裂控制设计[J].油气储运,2017,36(预出版):1.
 ZHANG Zhenyong,ZHANG Wenwei,ZHOU Yawei,et al.The fracture control design of the OD 1 422 mm buried pipeline in China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2017,36(9):1.
[9]赵园园,陈光联,宫爽.中俄东线黑龙江段地质灾害的特征及危险性[J].油气储运,2018,37(2):216.[doi:10.6047/j.issn.1000-8241.2018.02.015]
 ZHAO Yuanyuan,CHEN Guanglian,GONG Shuang.Characteristics and risk of geological disaster along China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2018,37(9):216.[doi:10.6047/j.issn.1000-8241.2018.02.015]
[10]毕光辉,任文明,曹阳,等.中俄东线黑龙江穿越管道安装设计方案[J].油气储运,2018,37(8):935.[doi:10.6047/j.issn.1000-8241.2018.08.015]
 BI Guanghui,REN Wenming,CAO Yang,et al.Pipeline installation design for Heilongjiang crossing of China-Russia Eastern Gas Pipeline[J].Oil & Gas Storage and Transportation,2018,37(9):935.[doi:10.6047/j.issn.1000-8241.2018.08.015]
[11]张振永,孟献强,孙学军,等.中俄东线站场工艺管道用高钢级低温钢管韧性指标[J].油气储运,2018,37(4):435.[doi:10.6047/j.issn.1000-8241.2018.04.012]
 ZHANG Zhenyong,MENG Xianqiang,SUN Xuejun,et al.Toughness index of low-temperature pipe of high steel grade used for the process pipelines at the station of China-Russia eastern natural gas pipeline[J].Oil & Gas Storage and Transportation,2018,37(9):435.[doi:10.6047/j.issn.1000-8241.2018.04.012]

备注/Memo

基金项目:中国石油天然气股份公司“十二· 五”重大科技专项“第三代大输量天然气管道关键技术研究”,2012E-2801-01。
作者简介:张振永,男,1971 年生,高级工程师,1995 年毕业于中国石油大学(华东)焊接设备及材料专业,现主要从事油气长输管道工程设计和管材可靠性评估等工作。地址:河北省廊坊市广阳区和平路146 号管道设计大厦,065000。电话:13292615649,Email:cppe_zhangzy@cnpc.com.cn

更新日期/Last Update: 2017-09-30