[1]叶帆,杨伟.塔河油田集输管道腐蚀与防腐技术[J].油气储运,2010,29(5):354-358,362.[doi:10.6047/j.issn.1000-8241.2010.05.011]
 Ye Fan and Yang Wei.Corrosion and Corrosion Control of Gathering Pipelines in Tahe Oilfield[J].Oil & Gas Storage and Transportation,2010,29(5):354-358,362.[doi:10.6047/j.issn.1000-8241.2010.05.011]
点击复制

塔河油田集输管道腐蚀与防腐技术

相似文献/References:

[1]陈迪.塔河油田原油集输管道弯管开裂原因[J].油气储运,2011,30(05):396.[doi:10.6047/j.issn.1000-8241.2011.05.021]
 Chen Di.Bended pipe cracking reason of gathering pipeline in Tahe Oilfield[J].Oil & Gas Storage and Transportation,2011,30(5):396.[doi:10.6047/j.issn.1000-8241.2011.05.021]
[2]赵金省,杨玲,魏美吉,等.苏里格气田输气管道清管周期的确定[J].油气储运,2011,30(01):71.[doi:10.6047/j.issn.1000-8241.2011.01.019]
 Zhao Jinsheng,Yang Ling,Wei Meiji,et al.Determination of pigging cycle for gas transmission pipeline in Sulige Gasfield[J].Oil & Gas Storage and Transportation,2011,30(5):71.[doi:10.6047/j.issn.1000-8241.2011.01.019]
[3]孙贵杰,齐安彬,张磊,等.聚乙烯管内插修复技术及其应用[J].油气储运,2011,30(07):530.[doi:10.6047/j.issn.1000-8241.2011.07.014]
 Sun Guijie,Qi Anbin,Zhang Lei,et al.Interpolation recovery technique of polyethylene pipe and its application[J].Oil & Gas Storage and Transportation,2011,30(5):530.[doi:10.6047/j.issn.1000-8241.2011.07.014]
[4]李自力,禹浩,程中海.长庆油田混输管道的结垢与防垢措施[J].油气储运,2011,30(02):133.[doi:10.6047/j.issn.1000-8241.2011.02.013]
 Li Zili,Yu Hao,Cheng Zhonghai.Scaling and anti-scaling in mixed transportation in Changqing oilfiled[J].Oil & Gas Storage and Transportation,2011,30(5):133.[doi:10.6047/j.issn.1000-8241.2011.02.013]
[5]石鑫,张志宏,刘强,等.塔河某单井管道频繁穿孔原因[J].油气储运,2011,30(11):848.[doi:10.6047/j.issn.1000-8241.2011.11.014]
 Shi Xin,Zhang Zhihong,Liu Qiang,et al.Reason analysis on the corrosion to leak pipeline of well[J].Oil & Gas Storage and Transportation,2011,30(5):848.[doi:10.6047/j.issn.1000-8241.2011.11.014]
[6]郑云萍,舒洁,李蕾,等.陆梁油田生产系统腐蚀影响因素的灰关联分析[J].油气储运,2010,29(10):774.[doi:10.6047/j.issn.1000-8241.2010.10.015]
 Zheng Yunping,Shu Jie,Li Lei.Grey Relational Analysis on Influence Factors of Corrosion in Production System of Luliang Oilfield[J].Oil & Gas Storage and Transportation,2010,29(5):774.[doi:10.6047/j.issn.1000-8241.2010.10.015]
[7]闫方平,任韶然.江苏油田W2断块防垢防腐复合技术的应用[J].油气储运,2009,28(10):59.[doi:10.6047/j.issn.1000-8241.2009.10.017]
 YAN Fangping,REN Shaoran.Application of Complex Technology on Scale and Corrosion Control in W2 Fault Block of Jiangsu Oilfield[J].Oil & Gas Storage and Transportation,2009,28(5):59.[doi:10.6047/j.issn.1000-8241.2009.10.017]
[8]杨静,叶帆.雅克拉气田集输管道腐蚀预测与防治[J].油气储运,2009,28(7):40.[doi:DOI:10.6047/j.issn.1000-8241.2009.07.012]
 YANG Jing,YE Fan.Prediction and Prevention of Corrosion in Gathering Lines of Yakela Condensate Gasfield[J].Oil & Gas Storage and Transportation,2009,28(5):40.[doi:DOI:10.6047/j.issn.1000-8241.2009.07.012]
[9]易成高,宫敬,杨勇,等.含二氧化碳天然气集输管道管材的优选[J].油气储运,2009,28(6):76.[doi:10.6047/j.issn.1000-8241.2009.06.022]
 YI Chenggao,GONG Jing.Optimal Selection of Steel Pipes for Gathering Pipelines Transporting CO2-contained Natural Gas[J].Oil & Gas Storage and Transportation,2009,28(5):76.[doi:10.6047/j.issn.1000-8241.2009.06.022]
[10]黄雪松,姜秀萍,刘强.油田集输管道介质多相流腐蚀数学模型研究[J].油气储运,2007,26(3):25.[doi:10.6047/j.issn.1000-8241.2007.03.007]
 HUANGA Xuesong,JIANG Xiuping.Study on Mathematical Model of Multiphase Flow in Gathering Pipeline of Oilfield[J].Oil & Gas Storage and Transportation,2007,26(5):25.[doi:10.6047/j.issn.1000-8241.2007.03.007]
[11]高淑红 张江江 张志宏 陈微.塔河油田集输管道内FeS 的形成及自燃风险[J].油气储运,2014,33(1):111.[doi:10.6047/j.issn.1000-8241.2014.01.024]
 GAO Shuhong,ZHANG Jiangjiang,ZHANG Zhihong,et al.GAO Shuhong, ZHANG Jiangjiang, ZHANG Zhihong, CHEN Wei[J].Oil & Gas Storage and Transportation,2014,33(5):111.[doi:10.6047/j.issn.1000-8241.2014.01.024]

备注/Memo

收稿日期:2009-6-19。
作者简介:叶帆,助理工程师,1980年生,2004年毕业于西南石油大学油气储运专业,现主要从事油气田腐蚀与防护的研究与技术应用工作. 电话:0991-3161112.E-mail:gcy.xbsj@sinopec.com

更新日期/Last Update: 1900-01-01