[1]谢文江,魏斌,陈娟利,等.含H2S/CO2气田油套管腐蚀与防护技术[J].油气储运,2010,29(2):93-96.[doi:10.6047/j.issn.1000-8241.2010.02.004]
 Xie Wenjiang,Wei Bin,Chen Juanli.Casing Steel Corrosion in H2S/CO2-contained Gas Field and Its Protection Technology[J].Oil & Gas Storage and Transportation,2010,29(2):93-96.[doi:10.6047/j.issn.1000-8241.2010.02.004]
点击复制

含H2S/CO2气田油套管腐蚀与防护技术

参考文献/References:

[1] Anne Marie K.Halvorsen,Terje Sontvedt.CO2 corrosion model for carbon steel:Including wall shear stress mode for multiphase flow and limits for production rate to avoid mesa attack[C]. Corrosion,Paper No.42,Houston:NACE1999.
[2] Schmitt G,Mueller M.Critical wall shear stresses in CO2 corrosion of carbon steel[C]. Corrosion.Paper No.44,Houston:NACE1999.
[3] Madan Gopal,Sathish Rajappa.Effect of multiphase slug flow on the stability of corrosion product layer[C]. Corrosion,paper No.46,Houston:NACE1999.
[4] Zeisel H,Durst F.Computation of erosion-corrosion processes in separated two-phase flows[C]. corrosion,Paper No.29,Houston:NACE1999.
[5] 林玉珍,刘景军,雍兴跃,等.数值计算法在流体腐蚀研究中的应用一层流条件下金属的腐蚀[J]. 中国腐蚀与防护学报,1999,19(1):1-7.

相似文献/References:

[1]谭羽非,曹琳,林涛.CO2作天然气地下储气库垫层气的可行性分析[J].油气储运,2006,25(3):12.[doi:DOI:10.6047/j.issn.1000-8241.2006.03.003]
 TAN Yufei,CAO Lin.Feasibility Analysis about Carbon Dioxide as Cushion Gas for Natural Gas Storage[J].Oil & Gas Storage and Transportation,2006,25(2):12.[doi:DOI:10.6047/j.issn.1000-8241.2006.03.003]
[2]赵青,李玉星.管道输送CO2准临界特性及安全控制[J].油气储运,2014,33(4):354.[doi:10.6047/j.issn.1000-8241.2014.04.003]
 ZHAO Qing,LI Yuxing.Quasi-critical characteristics and safety control of CO2 pipeline transportation[J].Oil & Gas Storage and Transportation,2014,33(2):354.[doi:10.6047/j.issn.1000-8241.2014.04.003]
[3]刘敏,李玉星,赵青,等.超临界CO2管道输送参数的敏感性分析[J].油气储运,2014,33(4):359.[doi:10.6047/j.issn.1000-8241.2014.04.004]
 LIU Min,LI Yuxing,ZHAO Qing,et al.Sensitivity analysis of transportation parameters of supercritical CO2 pipelines[J].Oil & Gas Storage and Transportation,2014,33(2):359.[doi:10.6047/j.issn.1000-8241.2014.04.004]
[4]齐国权,戚东涛,魏斌,等.非金属管在酸性环境应用存在的问题[J].油气储运,2015,34(12):1272.[doi:10.6047/j.issn.1000-8241.2015.12.004]
 QI Guoquan,QI Dongtao,WEI Bin,et al.Problems in application of non-metallic pipes in acidic environment[J].Oil & Gas Storage and Transportation,2015,34(2):1272.[doi:10.6047/j.issn.1000-8241.2015.12.004]
[5]张大同,滕霖,李玉星,等.管输CO2焦耳-汤姆逊系数计算方法[J].油气储运,2018,37(1):35.[doi:10.6047/j.issn.1000-8241.2018.01.007]
 ZHANG Datong,TENG Lin,LI Yuxing,et al.A calculation method for Joule-Thomson coefficient of pipeline CO2[J].Oil & Gas Storage and Transportation,2018,37(2):35.[doi:10.6047/j.issn.1000-8241.2018.01.007]
[6]张大同,滕霖,李玉星,等.高含CO2 的多相流体系节流效应模型[J].油气储运,2018,37(10):1128.[doi:10.6047/j.issn.1000-8241.2018.10.007]
 ZHANG Datong,TENG Lin,LI Yuxing,et al.Throttling effect model for multiphase flow system with high CO2 content[J].Oil & Gas Storage and Transportation,2018,37(2):1128.[doi:10.6047/j.issn.1000-8241.2018.10.007]
[7]刘宏波,王书淼,高铸,等.CO2、H2S对油气管道内腐蚀影响机制[J].油气储运,2007,26(12):43.[doi:10.6047/j.issn.1000-8241.2007.12.011]
 LIU Hongbo,WANG Shumiao.Study on the Internal Corrosion Mechanism of CO2,H2S to Oil Gas Pipelines[J].Oil & Gas Storage and Transportation,2007,26(2):43.[doi:10.6047/j.issn.1000-8241.2007.12.011]

备注/Memo

收稿日期:2009-12-2。
作者简介:谢文江,工程师,1981年生,2007年硕士毕业于西安理工大学材料加工工程专业,现从事油气田腐蚀与防护技术研究工作.电话:029-88726388.E-mail:xiewj@tgrc.org

更新日期/Last Update: 1900-01-01