[1]鹿锋华,孙增武,王辛夷.X65钢铜衬垫根焊工艺裂纹的敏感性[J].油气储运,2016,35(8):819-822.[doi:10.6047/j.issn.1000-8241.2016.08.004]
 LU Fenghua,SUN Zengwu,WANG Xinyi.Crack sensitivity of X65 steel root welding process with copper liners[J].Oil & Gas Storage and Transportation,2016,35(8):819-822.[doi:10.6047/j.issn.1000-8241.2016.08.004]
点击复制

X65钢铜衬垫根焊工艺裂纹的敏感性

参考文献/References:

[1] 肖健,郭晓疆,芦文发. 管道冷裂纹试验方法-TRC方法研究[J]. 焊管,2015,38(1):42-46. XIAO J,GUO X J,LU W F. Experimental exploration on TRC - A test method of cold crack in pipes[J]. Welded Pipe and Tube, 2015,38(1):42-46.
[2] 吴江桥,梁君直,王玮,等. 管道气动内对口器衬垫材料筛选试 验研究[J]. 石油工程建设,2009,35(2):10-12. WU J Q,LIANG J Z,WANG W,et al. Test research on choosing back-up material for pipeline pneumatic clamp[J]. Petroleum Engineering Construction,2009,35(2):10-12.
[3] 李冬玲,张勇,鹿锋华. 激光诱导击穿光谱法对焊接接头表面渗铜区铜元素的深度分布分析[J]. 冶金分析,2015,35(1):19-25. LI D L,ZHANG Y,LU F H. Depth distribution analysis of copper in copper infiltration zone of welding joint surface by laser induced breakdown spectrometry[J]. Metallurgical Analysis, 2015,35(1):19-25.
[4] 鹿锋华,周文波,姚海玉. X65 钢铜衬垫焊接工艺研究及应 用[J]. 焊接技术,2015,44(8):44-49. LU F H,ZHOU W B,YAO H Y. X65 steel copper liner welding process research and application[J]. Welding Technology,2015, 44(8):44-49.
[5] 梁君直,吴江桥,曾惠林,等. φ1219 带铜衬垫管道气动内对口器的研制[J]. 油气储运,2009,28(7):52-54. LIANG J Z,WU J Q,ZENG H L,et al. Development of φ1219 pneumatic internal clamp of pipelines with copper liners[J]. Oil & Gas Storage and Transportation,2009,28(7):52-54.
[6] 吴冰,陈辉. X80管线钢的焊接冷裂纹试验[J]. 电焊机,2008, 38(10):66-68. WU B,CHEN H. Research on cold cracks of welding X80 pipeline alloy steel[J]. Electric Welding Machine,2008,38(10):66-68.
[7] STAROSTIN V. Pipeline disaster in USSR. It had to happen,yet it could have been averted[J]. Pipes & Pipelines International, 1990,35(2):7-8.
[8] BIGNE F B. Laser-induced breakdown spectroscopy applications in the steel industry[J]. Spectrochimica Acta Part B,2008(3): 1122-1129.
[9] 罗智超,雷正龙. 长输管道外自动根焊采用铜衬垫焊接接头组织与性能分析[J]. 焊接,2014(12):42-47. LUO Z C,LEI Z L. Analysis of microstructure and performance on girth joint with copper back-up using automatic outside root welding for long-distance pipeline[J]. Welding & Joining, 2014(12):42-47.
[10] 梁君直,吴江桥,靳海成,等. 管道环焊缝采用铜衬垫根焊及焊缝渗铜研究[J]. 电焊机,2009,39(5):74-77. LIANG J Z,WU J Q,JIN H C,et al. Research on pipeline girth welding joint with copper infiltration and copper back-up shoes root welding[J]. Electric Welding Machine,2009,39(5): 74-77.
[11] 梁君直,黄福祥,邹欣,等. 带铜衬垫的管道环焊缝根焊技术及焊接工艺[J]. 电焊机,2009,39(5):83-86. LIANG J Z,HUANG F X,ZOU X,et al. Research of root welding technology and welding procedure with back-up shoes pipeline girth welding[J]. Electric Welding Machine,2009, 39(5):83-86.
[12] 荆雷. 油气管道焊接技术及发展前景[J]. 石油工业技术监督, 2008,12(11):21-24. JING L. Welding technology and development prospects for oil and gas pipeline[J]. Technology Supervision in Petroleum Industry,2008,12(11):21-24.

相似文献/References:

[1]梁君直,吴江桥,曾惠林.φ1219mm带铜衬垫管道气动内对口器的研制[J].油气储运,2009,28(7):52.[doi:DOI:10.6047/j.issn.1000-8241.2009.07.015]
 LIANG Junzhi,WU Jiangqiao.Development of φ1219 Pneumatic Internal Clamp of Pipelines with Copper Liners[J].Oil & Gas Storage and Transportation,2009,28(8):52.[doi:DOI:10.6047/j.issn.1000-8241.2009.07.015]
[2]鹿锋华 孙增武 王辛夷.X65 钢铜衬垫根焊工艺裂纹敏感性[J].油气储运,2016,35(预出版):1.
 LU Fenghua,SUN Zengwu,WANG X Y.Crack sensitivity of X65 steel root welding process with copper liners[J].Oil & Gas Storage and Transportation,2016,35(8):1.

备注/Memo

收稿日期:2015-5-6;改回日期:2015-11-1。
基金项目:中国石油天然气管道局科技攻关项目“海底管道铺管船法全自动焊接技术研究与应用”,2013-04-02。
作者简介:鹿锋华,男,工程师,1981 年生,2007 年硕士毕业于东北大学机械工艺制造及其自动化专业,现主要从事管道焊接工艺、焊接装备及其自动化方面的研究工作.地址:河北省廊坊市金光道44 号,065000.电话:18630629224,Email:lufenghua0402@126.com