[1]周道川 王艳婷.基于 BS7910 的焊缝缺陷剩余寿命分析方法[J].油气储运,2016,35(预出版):1-8.
 ZHOU Daochuan,WANG Yanting.Residual life analysis method of weld seam with defects based on BS7910[J].Oil & Gas Storage and Transportation,2016,35(预出版):1-8.
点击复制

基于 BS7910 的焊缝缺陷剩余寿命分析方法

相似文献/References:

[1]王雅芬 李荣光 冯少广 李莹 张鑫 李睿 王春明.CFRP 修复城市燃气管道焊缝缺陷的可行性[J].油气储运,2012,31(9):674.[doi:10.6047/j.issn.1000-8241.2012.09.007]
 Wang Yafen,Li Rongguang,Feng Shaoguang,et al.Feasibility of repairing urban gas pipeline weld defects by CFRP[J].Oil & Gas Storage and Transportation,2012,31(预出版):674.[doi:10.6047/j.issn.1000-8241.2012.09.007]
[2]张振永 郭彬 张金源. 西三线0.8 设计系数段环焊缝容许缺陷尺寸[J].油气储运,2013,32(10):1076.[doi:10.6047/j.issn.1000-8241.2013.10.009]
 Zhang Zhenyong,Guo Bin,Zhang Jinyuan. Tolerable flaw size of girth weld for the 3rd West-to-East Gas Pipeline with a design coefficient of 0.8[J].Oil & Gas Storage and Transportation,2013,32(预出版):1076.[doi:10.6047/j.issn.1000-8241.2013.10.009]
[3]周道川,王艳婷.基于BS 7910的焊缝缺陷剩余寿命分析方法[J].油气储运,2016,35(1):78.[doi:10.6047/j.issn.1000-8241.2016.01.015]
 ZHOU Daochuan,WANG Yanting.Residual life analysis method of weld seam with defects based on BS 7910[J].Oil & Gas Storage and Transportation,2016,35(预出版):78.[doi:10.6047/j.issn.1000-8241.2016.01.015]
[4]高喆慧,帅健,张思弘.管道焊缝缺陷的定量安全评定与容限尺寸[J].油气储运,2015,34(5):488.[doi:10.6047/j.issn.1000-8241.2015.05.006]